Adhesive Wear Behavior of Heat Treated Spheroidal Graphite Cast Iron
نویسندگان
چکیده
منابع مشابه
On the Effect of Pouring Temperature on Spheroidal Graphite Cast Iron Solidification
This work is focused on the effect of pouring temperature on the thermal-microstructural response of an eutectic spheroidal graphite cast iron (SGCI). To this end, experiments as well as numerical simulations were carried out. Solidification tests in a wedge-like part were cast at two different pouring temperatures. Five specific locations exhibiting distinct cooling rates along the sample were...
متن کاملStudy of the wear and friction behavior of immiscible as cast - Al - Sn / Graphite composite
In this paper we investigate the tribological properties of AlSn-based alloy with different amount of graphite at different normal loads and sliding speed. A modified impeller mixing coupled with chill casting technique was used for the preparation of immiscible alloys. In this paper Al-Sn binary alloys was chosen for this study. This binary system shows the miscibility gap at different concent...
متن کاملAuto-analysis system for graphite morphology of grey cast iron
The current method to classify graphite morphology types of grey cast iron is based on traditional subjective observation, and it cannot be used for quantitative analysis. Since microstructures have a great effect on the mechanical properties of grey cast iron and different types have totally different characters, six types of grey cast iron are discussed and an image-processing software subsys...
متن کاملLiterature search - Deteriorated Graphite Structures on Cast Iron Skins
The fatigue strength offerritic ductile iron, Grade EN-GJS-400-18U-LT. was determined for large section castings measuring 4 by 24 by 24 inches. Fatigue testing was conducted in bending fatigue in order to determine the influence of surface conditions on fatigue strength. Test specimens with various surface conditions were evaluated, including notched and un-notched specimens, as well as those ...
متن کاملTribological Behavior of Reinforced and Unreinforced High Chromium Cast Iron
In this paper, the metal matrix composites containing 22 wt % Cr, 2.5 wt % C and 2 to 16 volume percent TiC were processed by solidifying Fe-Cr-Ti-C in which precipitation of titaniumcarbide and chromium carbide occurred. The microstructure and abrasion resistance of in-situ synthesized composites were compared with the unreinforced high chromium white cast iron (HCWCI) containing 22 w. t. % C...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: IOP Conference Series: Materials Science and Engineering
سال: 2015
ISSN: 1757-899X
DOI: 10.1088/1757-899x/75/1/012003