All-solid-state silver batteries assembled by Spark Plasma Sintering

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Solid state sintering of very low and negative thermal expansion ceramics by Spark Plasma

Lithium aluminosilicate powder precursors of compositions Li2O:Al2O3:SiO2 as 1:1:2; and 1:1:3.11 were synthesized and sintered by the Spark Plasma Sintering technique. The sintering conditions were adjusted to obtain dense ceramic materials in an attempt to avoid the presence of a glassy phase. XRD and SEM images were employed for composition and microstructure characterization. The coefficient...

متن کامل

Spark Plasma Sintering As a Solid-State Recycling Technique: The Case of Aluminum Alloy Scrap Consolidation

Recently, "meltless" recycling techniques have been presented for the light metals category, targeting both energy and material savings by bypassing the final recycling step of remelting. In this context, the use of spark plasma sintering (SPS) is proposed in this paper as a novel solid-state recycling technique. The objective is two-fold: (I) to prove the technical feasibility of this approach...

متن کامل

Battery Materials for All - Solid State Batteries

The Grey group tackles a broad range of materials science and energy storage challenges that include various aspects of solid state chemistry, spectroscopy, and theoretical studies. To understand and control the materials that are desirable for energy storage applications, we use a suite of synthetic and analytical techniques, including diffraction, microscopy, solid state NMR, and computation....

متن کامل

Enhanced Multiferroic Properties of YMnO3 Ceramics Fabricated by Spark Plasma Sintering Along with Low-Temperature Solid-State Reaction

Based on precursor powders with a size of 200-300 nm prepared by the low-temperature solid-state reaction method, phase-pure YMnO₃ ceramics are fabricated using spark plasma sintering (SPS). X-ray diffraction (XRD) and scanning electron microscopy (SEM) reveal that the high-purity YMnO₃ ceramics can be prepared by SPS at 1000 °C for 5 minutes with annealing at 800 °C for 2 h. The relative densi...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Solid State Ionics

سال: 2012

ISSN: 0167-2738

DOI: 10.1016/j.ssi.2011.11.012