Anelastic deformation of a Pd40Cu30Ni10P20 bulk metallic glass during nanoindentation

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Rate dependence of serrated flow during nanoindentation of a bulk metallic glass

Plastic deformation of Pd–40Ni–20P bulk metallic glass (BMG) was investigated by instrumented nanoindentation experiments over a broad range of indentation strain rates. At low rates, the load–displacement curves during indentation exhibited numerous serrations or pop-ins, but these serrations became less prominent as the indentation rate was increased. Using the tip velocity during pop-in as a...

متن کامل

A Finite-Deformation Constitutive Model of Bulk Metallic Glass Plasticity

A constitutive model of bulk metallic glass (BMG) plasticity is developed which accounts for finitedeformation kinematics, the kinetics of free volume, strain hardening, thermal softening, rate-dependency and non-Newtonian viscosity. The model has been validated against uniaxial compression test data; and against plate bending experiments. The model captures accurately salient aspects of the ma...

متن کامل

Crystallization kinetics and glass-forming ability of bulk metallic glasses Pd40Cu30Ni10P20 and Zr41.2Ti13.8Cu12.5Ni10Be22.5 from classical theory

Due to their scientific significance and potential engineering applications, bulk metallic glasses are among the most intensively studied advanced materials. Understanding the glass-forming ability GFA of these metallic alloys is a long-standing subject. While a large number of empirical factors have been proposed to correlate with GFA of the alloys, a full understanding of GFA remains a goal t...

متن کامل

Deformation Mechanisms of Bulk Metallic Glass Matrix Composites

Bulk metallic glasses (BMGs) possess a unique set of mechanical properties that make them attractive structural materials: yield strength > 2 GPa, fracture toughness ~20 MPa.m and elastic strain limit ~2%. BMGs can also be cast into intricate shapes which retain their dimensional integrity and require no further machining. Unfortunately, monolithic BMGs fail catastrophically under unconstrained...

متن کامل

Ductile bulk metallic glass.

We report on experimental evidence of pronounced global plasticity measured in monolithic Pt57.5Cu14.7Ni5.3P22.5 bulk metallic glass under both bending and unconfined compression loading conditions. A plastic strain of 20% is measured, never before seen in metallic glasses. Also, permanent deformation and a strain exceeding 3% before failure is observed during bending of 4 mm thick samples. To ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied Physics Letters

سال: 2006

ISSN: 0003-6951,1077-3118

DOI: 10.1063/1.2198517