Atomic layer deposition of Pd nanoparticles on self-supported carbon-Ni/NiO-Pd nanofiber electrodes for electrochemical hydrogen and oxygen evolution reactions

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Pd nanoparticles on ZnO-passivated porous carbon by atomic layer deposition: an effective electrochemical catalyst for Li-O2 battery.

Uniformly dispersed Pd nanoparticles on ZnO-passivated porous carbon were synthesized via an atomic layer deposition (ALD) technique, which was tested as a cathode material in a rechargeable Li-O2 battery, showing a highly active catalytic effect toward the electrochemical reactions-in particular, the oxygen evolution reaction. Transmission electron microscopy (TEM) showed discrete crystalline ...

متن کامل

Controlled Synthesis of Pd/Pt Core Shell Nanoparticles Using Area-selective Atomic Layer Deposition

We report an atomic scale controllable synthesis of Pd/Pt core shell nanoparticles (NPs) via area-selective atomic layer deposition (ALD) on a modified surface. The method involves utilizing octadecyltrichlorosilane (ODTS) self-assembled monolayers (SAMs) to modify the surface. Take the usage of pinholes on SAMs as active sites for the initial core nucleation, and subsequent selective depositio...

متن کامل

A high-performance electrocatalyst for oxygen evolution reactions based on electrochemical post-treatment of ultrathin carbon layer coated cobalt nanoparticles.

Electrochemical post-treatment of ultrathin carbon layer coated cobalt nanoparticles generates a novel electrocatalyst, affording a small overpotential of 333 mV at a current density of 10 mA cm(-2) and a small Tafel slope of ∼58 mV per decade.

متن کامل

Application of Pd-Substituted Ni-Al Layered Double Hydroxides for the Hydrogen Evolution Reaction

Clean production of hydrogen from electrochemical water splitting has been known as a green method of fuel production. In this work, electrocatalytic hydrogen evolution reaction (HER) was investigated at new prepared layered double hydroxides (LDH) in acidic solution. NiAl/carbon black (CB) LDH was monitored using x-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, scannin...

متن کامل

Magnetic properties of Pd atomic chains formed during submonolayer deposition of 3d metals on Pd(110).

Recently, an unusual intermixing-driven scenario for the growth of atomic Pd chains on a Pd(110) surface during deposition of 3d metal atoms has been predicted (Stepanyuk 2009 Phys. Rev. B 79 155410) and confirmed by STM and STS experiments (Wie et al 2009 Phys. Rev. Lett. 103 225504). Performing ab initio calculations we demonstrate that Pd atomic chains grown above embedded Fe atoms exhibit m...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Colloid and Interface Science

سال: 2020

ISSN: 0021-9797

DOI: 10.1016/j.jcis.2020.02.063