Atomic Layer Deposition of Ultra-Thin Crystalline Electron Channels for Heterointerface Polarization at Two-Dimensional Metal-Semiconductor Heterojunctions

نویسندگان

چکیده

Atomic layer deposition (ALD) has emerged as a promising technology for the development of next generation low-power semiconductor electronics. The wafer-scaled growth two-dimensional (2D) crystalline nanostructures is fundamental step toward advanced nanofabrication technologies. Ga2O3 an ultra-wide bandgap metal oxide application in electronic devices. polymorphous with its unique characteristics and doping capabilities functional option heterointerface engineering at metal-semiconductor 2D heterojunctions technology. Plasma-enhanced atomic (PE-ALD) enabled ultra-thin low-growth temperatures. present study used PE-ALD process atomically thin ß-Ga2O3 films heterojunctions. Via control plasma gas composition ALD temperature, ~5.0 nm thick Au/Ga2O3-TiO2 heterointerfaces was achieved. Material characterization techniques showed effects temperature on properties structure films. following confirmed tunability this metal/semiconductor polarized junction, which works electron channel developed based tunable p-n junctions interfaces.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic/molecular layer deposition: a direct gas-phase route to crystalline metal-organic framework thin films.

Atomic/molecular layer deposition offers us an elegant way of fabricating crystalline copper(ii)terephthalate metal-organic framework (MOF) thin films on various substrate surfaces. The films are grown from two gaseous precursors with a digital atomic/molecular level control for the film thickness under relatively mild conditions in a simple and fast one-step process.

متن کامل

Atomic Layer Deposition of Noble Metal Thin Films

3 Preface 4 List of publications 5 List of symbols and abbreviations 6

متن کامل

Atomic Layer Deposition of Gallium Oxide Films as Gate Dielectrics in AlGaN/GaN Metal–Oxide–Semiconductor High-Electron-Mobility Transistors

In this study, films of gallium oxide (Ga2O3) were prepared through remote plasma atomic layer deposition (RP-ALD) using triethylgallium and oxygen plasma. The chemical composition and optical properties of the Ga2O3 thin films were investigated; the saturation growth displayed a linear dependence with respect to the number of ALD cycles. These uniform ALD films exhibited excellent uniformity a...

متن کامل

Graphene oxide monolayers as atomically thin seeding layers for atomic layer deposition of metal oxides.

Graphene oxide (GO) was explored as an atomically-thin transferable seed layer for the atomic layer deposition (ALD) of dielectric materials on any substrate of choice. This approach does not require specific chemical groups on the target surface to initiate ALD. This establishes GO as a unique interface which enables the growth of dielectric materials on a wide range of substrate materials and...

متن کامل

Metal-Insulator-Metal Single Electron Transistors with Tunnel Barriers Prepared by Atomic Layer Deposition

Single electron transistors are nanoscale electron devices that require thin, high-quality tunnel barriers to operate and have potential applications in sensing, metrology and beyond-CMOS computing schemes. Given that atomic layer deposition is used to form CMOS gate stacks with low trap densities and excellent thickness control, it is well-suited as a technique to form a variety of tunnel barr...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Coatings

سال: 2023

ISSN: ['2079-6412']

DOI: https://doi.org/10.3390/coatings13061041