Bonding properties of metals anodically bonded to glass

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Anodically bonded submicron microfluidic chambers.

We demonstrate the use of anodic bonding to fabricate cells with characteristic size as large as 7 x 10 mm(2), with height of approximately 640 nm, and without any internal support structure. The cells were fabricated from Hoya SD-2 glass and silicon wafers, each with 3 mm thickness to maintain dimensional stability under internal pressure. Bonding was carried out at 350 degrees C and 450 V wit...

متن کامل

Electrothermal Bonding of Carbon Nanotubes to Glass

Applications that exploit the exceptional properties of carbon nanotubes CNTs at practical length scales almost invariably involve the fundamental issues of nanotube-to-surface contacts; indeed, interface properties often dominate mechanical, electrical, and thermal performance in devices and materials based on CNTs. In this paper we present a method to attach CNTs to glass surfaces and investi...

متن کامل

Effect of diffusion bonding temperature on microstructure properties of Zr/Ti interlayer in the diffusion bonded joints of Zr702 to A516 steel

In this study, the effect of temperature on the microstructure and reactive layer at the interface between the Ti interlayer and the base metal related to the diffusion bonding of Zr702 to A516 low alloy steel was investigated. The joining was done using the spark plasma sintering technique at temperatures of 900, 950 and 1000°C for 30 minutes. Field Emission Scanning Electron Microscope (FESEM...

متن کامل

Effect of diffusion bonding temperature on microstructure properties of Zr/Ti interlayer in the diffusion bonded joints of Zr702 to A516 steel

In this study, the effect of temperature on the microstructure and reactive layer at the interface between the Ti interlayer and the base metal related to the diffusion bonding of Zr702 to A516 low alloy steel was investigated. The joining was done using the spark plasma sintering technique at temperatures of 900, 950 and 1000°C for 30 minutes. Field Emission Scanning Electron Microscope (FESEM...

متن کامل

Flexural Strength of Preheated Resin Composites and Bonding Properties to Glass-Ceramic and Dentin

To test the impact of preheating (25, 37, 54, or 68 °C) of TetricEvoCeram (TEC), FiltekSupremeXT (FSXT), and Venus (V) on flexural strength (FS), shear bond strength (SBS) and interfacial tension (IFT). FS was tested with TEC and FSXT. For SBS, glass-ceramic and human dentin substrate were fabricated and luted with the preheated resin composite (RC). SBSs of 1500 thermal cycled specimens were m...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Sensors and Actuators A: Physical

سال: 2004

ISSN: 0924-4247

DOI: 10.1016/j.sna.2003.10.070