Characterization of Superalloys by Artificial Neural Network Method

نویسندگان

چکیده

In this study, the use of artificial neural networks in classification a superalloys whose chemical analysis is performed quality process investigated. general, spectro method alone not sufficient to determine which class steel belongs to. addition method, tests such as tensile test, hardness test or notch impact are applied. The both take time and destroy material. fact that an algorithm classifies only according results used has made destructive mandatory. Artificial (ANNs), usually simply called (NNs), computing systems inspired by biological constitute animal brains. An ANN based on collection connected units nodes neurons, loosely model neurons brain. Each connection, like synapses brain, can transmit signal other neurons. our total 34 superalloy materials belonging 6 different classes were used. Chemical composition values determined for each sample. appropriate network was values. A predict material value been created. Weka 3.9.5 package program create model. high success rate prediction gave hope determination with method.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

scour modeling piles of kambuzia industrial city bridge using hec-ras and artificial neural network

today, scouring is one of the important topics in the river and coastal engineering so that the most destruction in the bridges is occurred due to this phenomenon. whereas the bridges are assumed as the most important connecting structures in the communications roads in the country and their importance is doubled while floodwater, thus exact design and maintenance thereof is very crucial. f...

runoff estimation using artificial neural network method

runoff is one of the major components of calculating water resource processes and is the main issue in hydrology. many concept models are used to predict the amount of runoff, which in most cases depend on topographical and hydrological data. conventional models are not appropriate for areas in which there is little hydrological data. changes in runoff are nonlinear, meaning it is time & space ...

متن کامل

Electrical Load Manageability Factor analyses by Artificial Neural Network Training

On typical medium voltage feeder, Load side management means power energy consumption controlling at connected loads. Each load has various amount of reaction to essential parameters variation that collection of these reactions is mentioned feeder behavior to each parameter variation. Temperature, humidity, and energy pricing variation or major event happening and power utility announcing to th...

متن کامل

Detecting Depression in Elderly People by Using Artificial Neural Network

Introduction: The possibility of depression is common in the elderly. Novel technologies allow us to monitor people related to depression. Hence, a model was provided to detect depression in elderly based on artificial neural network (ANN). Methods: The present study is an applied descriptive-survey research. Forty elderly people were randomly selected from the Elderly Care Center in Gonbad Ka...

متن کامل

Estimating Efficiency of Bank Branches by Dynamic Network Data Envelopment Analysis and Artificial Neural Network

Network data envelopment analysis models assess efficiency of decision-making unit and its sections using historical data but fail to measure efficiency of its units and their internal stages in the future. In this paper we aim to measure efficiency of stages of bank branches and obtain efficiency trend of stages during the time, then to estimate their efficiency in the future therefore we can ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: New trends in mathematical sciences

سال: 2022

ISSN: ['2147-5520']

DOI: https://doi.org/10.20852/ntmsci.2022.470