Cleavage fracture of two polystyrenes
نویسندگان
چکیده
منابع مشابه
Dissolution behavior of fluoroalcohol substituted polystyrenes
α-Fluoroalcohols have been proposed as transparent, base-soluble functional groups for use in the design of new 157 nm photoresist polymers. The two most common and easily prepared fluoroisopropanol groups are bis-trifluoromethyl carbinols (hexafluoroalcohol) and methyl-trifluoromethyl carbinols (trifluoroalcohol). This paper describes studies designed to assess the suitability of both of these...
متن کاملTreatment of a Mandibular Fracture by Two Perpendicular Mini-Plates
Introduction: In open reduction and internal fixation for the treatment of mandibular fracture, the fixation technique used is very important in reducing post-operative complications and promoting the healing process. This study assessed the results of fixation of the mandible using two mini-plates perpendicular to each other in the lower border of the mandible for fracture treatment. Materi...
متن کاملTwo Cases of Fracture
into the 1st Surgeon's Ward of the Medical College Hospital on the 25th March, 1866, at 9 p. m., with fractured ribs ; the fracture extending from the apex of the left axilla, downwards and forwards, to the margin of the costal cartilages, below the left nipple, involving therefore all the ribs situated in that line, i. e., from the third to the eighth vib. There was emphysema of the left side ...
متن کاملEffect of phosphorus on cleavage fracture in -carbide
To understand the origin of cleavage fracture which dominates in Fe Mn -Al-C alloys at a high phosphorus concentration, we performed first-principles study of the phosphorus effect on ideal cleavage energy and critical stress in -carbide, Fe3AlC, a precipitate in the austenitic alloys. We find that phosphorus has higher solubility in Fe3AlC than in -Fe and sharply reduces the cleavage character...
متن کاملDirectional anisotropy in the cleavage fracture of silicon
Total-energy pseudopotential calculations are used to study the cleavage anisotropy in silicon. It is shown that cracks propagate easily on 111 and 110 planes provided crack propagation proceeds in the <1;10> direction. In contrast, if the crack is driven in a <001> direction on a 110 plane the bond breaking process is discontinuous and associated with pronounced relaxations of the surrounding ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Applied Polymer Science
سال: 1974
ISSN: 0021-8995,1097-4628
DOI: 10.1002/app.1974.070180727