Cobalt-based superalloy layers deposited on X38CrMoV5 steel base metal by explosion cladding process

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Nickel-based Superalloy Layer Deposited on AISI H13 Hot Tool Steel Base Metal Using Explosion Cladding process

An experimental test was carried out to explosively clad solution annealed Inconel 718 superalloy on quench-tempered AISI H13 hot tool steel. A wavy with vortices interface geometry was obtained from this experiment. A gradual change in the wavelength along the direction of welding was observed which was due to a change in the impact angle, following the plate contacts. In this paper, the exper...

متن کامل

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

Structural Analysis of Three-metal Explosion Joint: Zirconium-titanium-steel

Explosion metal welding is high-speed angle oblique collision of two or more metal plates caused by detonation. The metal is joined – welded under high dynamic pressure creating by plastic deformation the waves on the bond interface, accompanied by local adiabatic heating 1 . The explosive metal cladding process can be divided into three stages: a) generation of explosion energy through the det...

متن کامل

Flow Stress Modeling in a γ-γ/ Cobalt Base Superalloy by Using the Hyperbolic Sine Equation and ANN Method

The new class of wrought γ-γ/ Co-base superalloys, which are based on Co-Al-W system,  was developed by conventional hot working routes with a high volume fraction of γ/ precipitates and good mechanical properties. The aim of the present study was to predict the flow stress and hot deformation modeling of a novel γ-γ/ Co-base superalloy. The hot compression test...

متن کامل

Layers of Metal Nanoparticles on Semiconductors Deposited by Electrophoresis from Solutions with Reverse Micelles

Pd nanoparticles were prepared with reverse micelles of water/AOT/isooctane solution and deposited onto silicon or InP substrates by electrophoresis. A large change of capacitance-voltage characteristics of mercury contacts on a semiconductor was found after Pd deposition. This change could be modified when the Pd deposition is followed by a partial removal of the deposited AOT. The deposited P...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Surface and Coatings Technology

سال: 2008

ISSN: 0257-8972

DOI: 10.1016/j.surfcoat.2007.12.008