Correlation of spherical nanoindentation stress-strain curves to simple compression stress-strain curves for elastic-plastic isotropic materials using finite element models

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Modifying Stress-Strain Curves Using Optimization and Finite Elements Simulation Methods

Modifying stress-strain curves is one of the important topics in mechanical engineering and materials science. Real stress-strain curves should be modified after necking point as stress becomes three-dimensional after creation of throat, and consequently, equivalent stress should be used instead of axial one. Also, distribution of triple stresses across throat section is not uniform anymore, an...

متن کامل

Correcting the stress-strain curve in hot compression test using finite element analysis and Taguchi method

In the hot compression test friction has a detrimental influence on the flow stress through the process and therefore, correcting the deformation curve for real behavior is very important for both researchers and engineers. In this study, a series of compression tests were simulated using Abaqus software. In this study, it has been employed the Taguchi method to design experiments by the factor...

متن کامل

Deformation micromechanisms of ZnO single crystals as determined from spherical nanoindentation stress– strain curves

The following item is made available as a courtesy to scholars by the author(s) and Drexel University Library and may contain materials and content, including computer code and tags, artwork, text, graphics, images, and illustrations (Material) which may be protected by copyright law. Unless otherwise noted, the Material is made available for non profit and educational purposes, such as researc...

متن کامل

On the measurement of stress–strain curves by spherical indentation

It has been proposed that with the appropriate models, instrumented indentation test (IIT) data can be reduced to yield the uniaxial stress–strain behavior of the test material. However, very little work has been done to directly compare the results from uniaxial tension and spherical indentation experiments. In this work, indentation and uniaxial tension experiments have been performed on the ...

متن کامل

Investigation of Stress-Strain Behavior of Plastic Concrete Using Monotonic Triaxial Compression Tests

In this paper, the mechanical behavior of plastic concrete being used in the cut-off walls of earth dams has been studied. To do the task, triaxial compression tests on the specimens in various ages and mix designs under different confining pressures have been done and the stress-strain behavior of such materials and their strength parameter changes has been experimentally investigated. It has ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Materialia

سال: 2016

ISSN: 1359-6454

DOI: 10.1016/j.actamat.2016.04.034