Corrosion Behavior and Galvanic Corrosion Resistance of WC and Cr3C2 Cermet Coatings in Madeira River Water

نویسندگان

چکیده

Thermally sprayed cermet coatings are adequate solutions to improve cavitation and wear resistance of hydraulic turbines made stainless steel (SS), especially in rivers with a high sediment load, such as the Madeira River Brazil. However, some cermets easily dissolved river water, leading premature failure coating costly maintenance. Moreover, galvanic corrosion induced by coupling SS can accelerate dissolution. Therefore, six (WC-12Co, WC-10Ni, WC-10Co-4Cr, Cr3C2-25NiCr, Cr3C2-10NiCr Cr3C2-10Ni) these materials coupled CA6NM were evaluated solution that simulated water. WC-12Co WC-10Ni exhibited highest rates, 0.077 0.068 mm/year, respectively, whereas Cr content WC-10Co-4Cr (0.017 mm/year) Cr3C2-based (0.005 0.007 led them corrode at slower rates. negligible current when SS, making good options coat turbines. In contrast, underwent more severe process, which would drastically reduce lifespan turbine coatings.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Galvanic Corrosion Behavior of Dental Alloys

There is a wide variety of dental alloys, ranging from nearly pure gold and conventional gold-based alloys to alloys based on silver, palladium, nickel, cobalt, iron, titanium, tin, and other metals (Table 1). The types of dental alloys have increased significantly since 1980s in order to change the market price of gold and palladium. Although gold alloys are the mate‐ rials of choice in this a...

متن کامل

Investigation of Corrosion Behavior and Galvanic Corrosion Simulation of Super Duplex Stainless Steel UNS S32750 Weld Zone

Galvanic corrosion is an ever-present problem in all different environments, particularly in tanks. The goal of this project is to develop a finite element model that can be used with experimental data to characterize the corrosion of a galvanic weldments couple in an electrolyte. In this study sample are welded by gas tungsten arc welding and friction stir welding. According to ASTM G8, Evalua...

متن کامل

Investigation of Corrosion Behavior and Galvanic Corrosion Simulation of Super Duplex Stainless Steel UNS S32750 Weld Zone

Galvanic corrosion is an ever-present problem in all different environments, particularly in tanks. The goal of this project is to develop a finite element model that can be used with experimental data to characterize the corrosion of a galvanic weldments couple in an electrolyte. In this study sample are welded by gas tungsten arc welding and friction stir welding. According to ASTM G8, Evalua...

متن کامل

High-temperature Corrosion Behavior of Iron Aluminide Alloys and Coatings

A multi-year effort has been focused on optimizing the long-term oxidation performance of ingot-processed (IP) and oxide-dispersion strengthened (ODS) Fe3Al and iron aluminidebased coatings. Based on results from several composition iterations, a Hf-doped alloy (Fe28Al-2Cr-0.05at.%Hf) has been developed with significantly better high temperature oxidation resistance than other iron aluminides. ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Thermal Spray Technology

سال: 2021

ISSN: ['1059-9630', '1544-1016']

DOI: https://doi.org/10.1007/s11666-021-01152-8