Cover Feature: Atomic Layer Deposition of Ternary Indium/Tin/Aluminum Oxide Thin Films, Their Characterization and Transistor Performance under Illumination. (Chem. Eur. J. 38/2021)

نویسندگان

چکیده

Lesser is better: Multilayered heterostructures comprising of In2O3, SnO2, and one or two atomic layers Al2O3 were studied for their application in thin-film transistors (TFT). The cover image centers around the fabrication a multilayer thin film oxide aggregate which works as semiconductor transistor device. It composed different In2O3 fabricated using layer deposition (ALD) technique employs reaction suitable organometallic precursors with water, all originate from gas phase an individual molecular source (left upper side). rainbow reflects stability material against illumination. background depicts universal binary 0/1 code representing every-day use our modern society. More information can be found Full Paper by J. Schneider et al. (DOI: 10.1002/chem.202101126).

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic layer deposition and properties of ZrO2/Fe2O3 thin films

Thin solid films consisting of ZrO2 and Fe2O3 were grown by atomic layer deposition (ALD) at 400 °C. Metastable phases of ZrO2 were stabilized by Fe2O3 doping. The number of alternating ZrO2 and Fe2O3 deposition cycles were varied in order to achieve films with different cation ratios. The influence of annealing on the composition and structure of the thin films was investigated. Additionally, ...

متن کامل

Atomic Layer Deposition of Noble Metal Thin Films

3 Preface 4 List of publications 5 List of symbols and abbreviations 6

متن کامل

Atomic Layer Deposition of Tin Monosulfide Thin Films

Thin film solar cells made from earth-abundant, non-toxic materials are needed to replace the current technology that uses Cu(In,Ga)(S,Se)2 and CdTe, which contain scarce and toxic elements. One promising candidate absorber material is tin monosulfide (SnS). In this report, pure, stoichiometric, single-phase SnS films were obtained by atomic layer deposition (ALD) using the reaction of bis(N,N’...

متن کامل

Atomic/molecular layer deposition of hybrid inorganic-organic thin films

Aalto University, P.O. Box 11000, FI-00076 Aalto www.aalto.fi Author Pia Sundberg Name of the doctoral dissertation Atomic/molecular layer deposition of hybrid inorganic-organic thin films Publisher School of Chemical Technology Unit Department of Chemistry Series Aalto University publication series DOCTORAL DISSERTATIONS 201/2014 Field of research Inorganic Chemistry Manuscript submitted 11 Se...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Chemistry: A European Journal

سال: 2021

ISSN: ['0947-6539', '1521-3765']

DOI: https://doi.org/10.1002/chem.202102030