Creep and Mechanical Behavior Study of Inconel 718 Superalloy

نویسندگان

چکیده

Over the years, demand for high engine efficiency has resulted in development of new generation superalloys with improved elevated temperature properties, especially creep resistance. This study aimed to evaluate and mechanical behavior Inconel 718 superalloy. Creep tests were performed at range 650 700 °C stress 625 814 MPa. Hot tensile oxidation characterization techniques used this scanning electron microscopy (SEM) microstructural fracture surface analysis, transmission (TEM) precipitates analysis; grazing X-ray diffraction analysis oxide formation Vickers microhardness. The analyze exponent value (n = 36.48) activation energy (Qc 512.97 kJ/mol), suggested that mechanism was climb dislocation mechanism. presented ductile intergranular 675 °C.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Investigation of Cutting Forces Superalloy Inconel 718

Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...

متن کامل

Characterization of strain induced precipitation in Inconel 718 superalloy

Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...

متن کامل

Effect of Thermomechanical Working on the Microstructure and Mechanical Properties of Hot Pressed Superalloy Inconel 718

Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...

متن کامل

Ultrasonic assisted creep feed grinding of Inconel 718

The paper details the effects of depth of cut and vibration amplitude when ultrasonic assisted (US) creep feed grinding Inconel 718 with an open structured alumina based wheel. The workpiece was actuated at a constant frequency (~20.5kHz) via a block sonotrode attached to a 1kW piezoelectric transducer-generator system. A full factorial experimental array comprising 12 tests was conducted invol...

متن کامل

Evaluation of Tool Performance With Nanocrystalline Multilayer Coatings on the Machinability of Superalloy Inconel 718

In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machinin...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Research-ibero-american Journal of Materials

سال: 2022

ISSN: ['1980-5373', '1516-1439']

DOI: https://doi.org/10.1590/1980-5373-mr-2021-0280