Creep of Ni-Al and Ni-Cr-Al Superalloy Foams

The steady-state creep rate of Ni-base metallic foams, with superalloy composition (in wt. pct) Ni7.8∼9.1Al (relative density, ρ = 2.5-2.6) and Ni-13.5∼16.6Cr-5.1∼8.9Al (ρ = 2.8∼3.0), was measured under a range of temperatures (680∼825°C) and applied stresses (0.1∼0.3 MPa), and compared with that of NiAl intermetallic foams (ρ = 5.3). The stress exponent and activation energy are within the exp...

متن کامل

Modeling the Temperature-dependence of Tertiary Creep Damage of a Directionally Solidified Ni-base Superalloy

Directionally solidified (DS) Ni-base superalloys have become a commonly used material in gas turbine components. Controlled solidification during the material manufacturing process leads to a special alignment of the grain boundaries within the material. This alignment results in different material properties dependent on the orientation of the material. When used in gas turbine applications t...

متن کامل

Creep Crack Growth Simulation of Ni-base Superalloy

The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...

متن کامل

Nondestructive Evaluation of the Creep Damaged Ni-Based Superalloy Using Ultrasonic Wave Method

The effects of microstructures during creep on the ultrasonic attenuation have been investigated for Ni based superalloy (IN738LC). The cuboidal γ′ precipitates in the virgin material became coarsened preferentially in the direction perpendicular to the applied stress axis as creep time increased. The length of γ′ precipitates increased with creep time, while the width increased slightly. The i...

متن کامل

TENSION/COMPRESSION ASYMMETRY IN CREEP BEHAVIOR OF A Ni-BASED SUPERALLOY

Orientation and temperature dependence of yield stress or CRSS (Critical Resolved Shear Stress) and tension/compression anisotropy of the yield stress or CRSS have been shown by Shah and Duhl (1), Heredia and Pope (2), and Miner et al. (3). Tension/compression asymmetry in the yield strength of Ni-based superalloys has been explained in terms of the “core width effect” (4). Shah and Duhl (5) ob...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Progress in Natural Science: Materials International

سال: 2012

ISSN: 1002-0071

DOI: 10.1016/j.pnsc.2012.07.005