Crystal plasticity modeling of non-Schmid yield behavior: from Ni<sub>3</sub>Al single crystals to Ni-based superalloys

نویسندگان

چکیده

A Crystal Plasticity Finite Element (CPFE) framework is proposed for modeling the non-Schmid yield behavior of L12 type Ni3Al crystals and Ni-based superalloys. This relies on estimation model parameters directly from orientation- temperature-dependent experimental stress data. The inelastic deformation extended to precipitate phase superalloys in a homogenized dislocation density based crystal plasticity framework. used simulate single superalloy, CMSX-4, temperature range 260-1304 K. Model predictions are general agreement with experiments. also made regarding tension-compression asymmetry dominant slip mechanism at over standard stereographic triangle various temperatures both these materials. These provide valuable insights underlying (orientation- temperature-dependent) mechanisms yield. In this regard, may serve as standalone analytical predicting stress, function orientation temperature.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Aspects of Non-associated Single Crystal Plasticity: Influence of Non-schmid Effects and Localization Analysis

Abstract--The aim of this work is the consideration of so-called non-Schmid effects within nonassociated single crystal plasticity at small strains. To this end, two additional activating mechanisms for dislocation flow on a slip system are modelled. For convenience the corresponding algorithmic setting is discussed in the sequel. Next, the influence of non-Schmid effects and non-associativity ...

متن کامل

Physics Based-crystal Plasticity Modeling of Single Crystal Niobium

Physics Based-crystal Plasticity Modeling of Single Crystal Niobium

متن کامل

Femtosecond Laser Micromachining of Single-crystal Superalloys

Investigations on femtosecond laser micromachining of single crystal superalloys with and without plasma-sprayed thermal barrier coatings were conducted under laser fluences ranging from 0.1 J/cm up to 160 J/cm. Micromachining was carried out in air using a titanium:sapphire laser system ( = 780 nm) operating at a repetition rate of 1 kHz and delivering individual pulses of ~150 fs duration. Th...

متن کامل

Mechanism-based Constitutive Modeling of L12 Single-crystal Plasticity

Ni 3Al, an L12 structure intermetallic crystal, is the basic composition of the y' precipitates in nickel-based superalloys and is a major strengthening mechanism contributing to the superalloys' outstanding high-temperature mechanical properties. Many L12-structure crystals present unusual macroscopic mechanical properties, including the anomalous temperature-dependence of yield strength and s...

متن کامل

Near-tip closure and cyclic plasticity in Ni-based single crystals

Fatigue crack growth was investigated in a 001 1⁄2 oriented single crystal specimen, made of a Ni-based superalloy, Haynes 230. Crack propagation was characterized with digital image correlation: crack closure, measured by analyzing the relative displacements of crack flanks, showed closure levels much lower than polycrystal alloys. Reversed plastic zones were calculated from regressed stress i...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Modelling and Simulation in Materials Science and Engineering

سال: 2021

ISSN: ['1361-651X', '0965-0393']

DOI: https://doi.org/10.1088/1361-651x/abd621