Current Fractographic Research and Its Application. I: Fatigue Fracture.

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

construction and validation of translation metacognitive strategy questionnaire and its application to translation quality

like any other learning activity, translation is a problem solving activity which involves executing parallel cognitive processes. the ability to think about these higher processes, plan, organize, monitor and evaluate the most influential executive cognitive processes is what flavell (1975) called “metacognition” which encompasses raising awareness of mental processes as well as using effectiv...

Thermal Stress Resistance to Fracture and its Relation to with Resistance to Thermal Fatigue and Shock

Dense Silicon nitride was investigated to determine the effect of its microstructural parameters and densification on thermo-mechanical properties and thermal stress resistance to fracture initiation during a hot or cold mechanical and thermal shock testing. The different materials and microstructures were obtained by changing the parameters such as the type of the powder, additive, forming p...

متن کامل

Thermal Stress Resistance to Fracture and its Relation to with Resistance to Thermal Fatigue and Shock

Dense Silicon nitride was investigated to determine the effect of its microstructural parameters and densification on thermo-mechanical properties and thermal stress resistance to fracture initiation during a hot or cold mechanical and thermal shock testing. The different materials and microstructures were obtained by changing the parameters such as the type of the powder, additive, forming p...

متن کامل

Fatigue of Yttria-Stabilized Zirconia: I, Fatigue Damage, Fracture Origins, and Lifetime Prediction

Uniaxial tension-compression fatigue behavior of 3-mol%yttria-stabilized tetragonal zirconia polycrystals was investigated. Hysteresis in the stress-plastic strain curve featured cumulative plastic strain and weakened elastic stiffness. Fracture statistics in terms of cycle-to-failure depends strongly on the maximum stress and less on the stress amplitude. Preexisting processing flaws were iden...

متن کامل

Cyclic Fatigue Resistance and Fractographic Analysis of Race and Protaper Rotary NiTi Instruments

INTRODUCTION This study investigated the fatigue and fracture modes of RaCe and ProTaper rotary instruments. MATERIALS AND METHODS Fatigue resistance was evaluated by rotating the files 30° or 60° and with 2 or 5mm radius of curvature. RaCe taper 06 size 25 and ProTaper F1 files (n=40) were used. The number of rotations to failure was analyzed by two-way ANOVA and independent sample t-test. F...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1998

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.47.637