Hot deformation behavior and the microstructural evolution of Inconel 625 superalloy plates are investigated by hot compression tests in a range working temperatures (800–1050 °C) strain rates (0.001–1 s−1). The observation shows that strong <110> texture forms when processing temperature is below 950 °C, whose intensity decreases with increases temperature, it disappears compressing above °C. During test, twin-related dynamic recrystallization (DRX) occurs range, DRX temperature. In addition, as increases, continuum decreases.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microstructural Evolution of X45CrNiW189 Valve Steel During Hot Deformation

The hot compression tests were carried on X45CrNiW189 valve steel (X45) in the temperature range of 1000– 1200 °C and the strain rate range of 0.004 – 0.5 s-1 in order to study the high temperature softening behavior of this steel. For the exact prediction of flow stress, the effective stress-effective strain curves were obtained from experiments under various conditions. On the basis of experi...

متن کامل

microstructural evolution of x45crniw189 valve steel during hot deformation

the hot compression tests were carried on x45crniw189 valve steel (x45) in the temperature rangeof 1000– 1200 °c and the strain rate range of 0.004 – 0.5 s-1 in order to study the high temperaturesoftening behavior of this steel. for the exact prediction of flow stress, the effective stress-effectivestrain curves were obtained from experiments under various conditions. on the basis of experimen...

متن کامل

Hot Deformation Behavior of Ni80A Superalloy During Non-Isothermal Side Pressing

In the present study, the microstructural changes of a Nickel based superalloy Nimonic80A during a non-isothermal deformation were studied. Therefore, microstructure evolutionduring hot side pressing test was predicted with combined methods of finite element analysis andprocessing map of the material. The predicted results were validated through experimentalmicrostructural studies. The results ...

متن کامل

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

متن کامل

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2021

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met11050824