Delamination Strength Evaluation of Thermal Sprayed Coating by Torsion Pin-Test Method
نویسندگان
چکیده
منابع مشابه
Evaluation of the Shearing Strength of a WC-12Co Thermal Spray Coating by the Scraping Test Method
This paper reports on an experimental and analytical investigation conducted into efficacy of the scraping shear-test method in estimating the shearing adhesive strength of a thermally sprayed coating. It was found that the critical average shear stress, the apparent failure strength of WC-Co thermal spray coating, depends on both the dimensions of the test piece and the loading position around...
متن کاملEffect of Surface Roughness Morphology on Bond Strength of Thermal Sprayed WC-10Co-4Cr Ceramic/Metal Coating
In this study, the effect of surface roughness and roughness morphology on the bond strength of WC-Co-Cr coatings has investigated. The three different surfaces morphology are use for this purpose. The first and tow samples sandblasted with alumina and silicon carbide respectively. Other sample no sandblasted before spraying process. The same WC-10Co-4Cr coating deposited on the substrates with...
متن کاملHigh-temperature degradation of plasma sprayed thermal barrier coating systems
Thermal barrier coating systems (TBCs) are used in gas turbines to prevent high-temperature degradation of metallic materials in the combustor and turbine. One of the main concerns regarding TBCs is poor reliability, and accurate life prediction models are necessary in order to fully utilise the beneficial effects of TBCs. This research project aims at developing deeper understanding of the deg...
متن کاملInfluence on Thermal Barrier Coating Delamination Behaviour of Edge Geometry
Ceramic thermal barrier coatings are commonly used in gas turbine hot components (e.g., combustor liners/buckets and guide vane platforms). In components that are only partially coated or have cooling-air outlets, coating-end stress singularities may lead to the spallation of the coating. Depending on the geometry of the transition from coated to uncoated material, the severity of the stress si...
متن کاملMonitoring Delamination of Plasma-Sprayed Thermal Barrier Coatings by Reflectance-Enhanced Luminescence
Highly scattering plasma-sprayed thermal barrier coatings (TBCs) present a challenge for optical diagnostic methods to monitor TBC delamination because scattering attenuates light transmitted through the TBC and usually degrades contrast between attached and delaminated regions of the TBC. This paper presents a new approach where reflectance-enhanced luminescence from a luminescent sublayer inc...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Solid Mechanics and Materials Engineering
سال: 2011
ISSN: 1880-9871
DOI: 10.1299/jmmp.5.1042