Determination of Fracture Toughness for Whisker-Reinforced Aluminium Alloy Matrix Composite using Chevron-Notched Specimen

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluation of Cleavage Fracture Toughness for Steel by Chevron-Notched Specimen

Fracture toughness tests were conducted for an A533B-1 steel by using chevron-notched compact specimens in the temperature range from the lower shelf regime up to the transition temperature in order to assess the R-curve for cleavage fracture. The applicability of these specimens to the simple fracture toughness test without introducing fatigue pre-cracks was examind. The following are the summ...

متن کامل

STRENGTH AND FRACTURE TOUGHNESS OF WHISKER REINFORCED DENTAL RESIN-BASED COMPOSITES

Enhancing the properties of dental resin composites is of interest to researchers. The objective of the present investigation was to improve the strength and fracture toughness of dental composites via addition of silicon carbide whiskers and substitution of commonly used filler materials with stabilized zirconia ceramic powder. It was also intended to study the effect of powder- to- whisker ra...

متن کامل

Evaluation Method of Fracture Properties of Fiber-reinforced Self-healing Ceramics

ID No. : FC-168 ABSTRACT Fiber-reinforced self-healing ceramic (shFRC) [1] is considered to be most attractive candidate of next generation structural materials using at high temperature, e.g. turbine blade, exhaust component of car engine etc. The shFRCs consist of three components, which are oxide fiber bundle, oxide matrix and self-healing agent interlayer. As the self-healing is generated a...

متن کامل

Microstructure and Fracture Toughness of Hot-Pressed Silicon Carbide Reinforced with Silicon Carbide Whisker

The effects of p-Sic whisker addition on the microstructural evolution and fracture toughness (K,c) of hot-pressed SIC were investigated. Most of the whiskers added disappeared during the densification process by transformation into the a-phase. The remaining whiskers acted as nuclei for grain growth, resulting in the formation of large tabular grains around the whiskers. The tabular grains aro...

متن کامل

TENSILE AND FRACTURE CHARACTERISTICS OF A SIC- PARTICLE-REINFORCED 7075 ALUMINIUM ALLOY

Fracture behavior of a 7075 aluminium alloy reinforced with 15 Vol%. SiC particles was studied after T6 and annealing heat treatments under uniaxial tensile loading at room temperature. The scanning electron microscopy of fractured surfaces and EDS analysis showed:, that fracture mechanism changed from due mainly to fractured particle in T6 condition to interface decohesion in samples in anneal...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: JSME international journal. Ser. 1, Solid mechanics, strength of materials

سال: 1991

ISSN: 0914-8809

DOI: 10.1299/jsmea1988.34.2_234