Determining the constitutive behavior of nonlinear visco-elastic-plastic PMMA thin films using nanoindentation and finite element simulation

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Simulation of Plastic Deformation Behavior of Ti-6Al-4V Alloy by Finite Element Method

Mechanical properties of alloys have a strong relation with microstructure and determination of their behavior can lead to multiple advantages. To obtain this goal, finite element method )FEM( is one of the best ways. In this study a series of experiments were carried out on the produced Ti-6Al-4V to obtain its mechanical characteristics and to prepare it for photographing in micro dimensions. ...

متن کامل

Axial Crushing Analysis of Sandwich Thin-walled Tubes using Experimental and Finite Element Simulation

Application of impact energy absorption systems in different industries is of special significance. Thin-walled tubes, due to their lightness, high energy absorption capacity, long crushing length and the high ratio of energy absorption to weight, have found ever-increasing application as one of the most effective energy absorption systems. In this research, through  carrying out experimental t...

متن کامل

Finite element simulation of the effect of surface roughness on nanoindentation of thin films with spherical indenters

The effect of the surface roughness on nanoindentation results was investigated instancing a series of CrN thin films deposited by unbalanced magnetron sputtering. The arithmetic roughness (Ra) of the films ranged between 2 and 10 nm and was measured by atomic force microscopy. The measured surface topography was incorporated into a finite element model, which allowed simulating the indentation...

متن کامل

Finite element modeling of nanoindentation to extract load-displacement characteristics of bulk materials and thin films

The finite element modeling (FEM) technique has been applied to study the loading-unloading characteristics, stress and strain fields of the bulk materials such as titanium, iron, copper and thin films of titanium and copper subjected to Berkovich nanoindentation process. The loading and unloading curves obtained from numerical simulation results are compared with the curves obtained earlier th...

متن کامل

Determining the elastic modulus and hardness of an ultra-thin film on a substrate using nanoindentation

A data analysis procedure has been developed to estimate the contact area in an elasto-plastic indentation of a thin film bonded to a substrate. The procedure can be used to derive the elastic modulus and hardness of the film from the indentation load, displacement, and contact stiffness data at indentation depths that are a significant fraction of the film thickness. The analysis is based on Y...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials & Design

سال: 2021

ISSN: 0264-1275

DOI: 10.1016/j.matdes.2020.109239