Differential Scanning Calorimetric Studies of Poly (Methyl Methacrylate Co-Styrene (MMA-Co-ST) Copolymers

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Calorimetric study of block-copolymers of poly(n-butyl acrylate) and gradient poly(n-butyl acrylate-co-methyl methacrylate)

The nanophase separation in diblock and triblock copolymers consisting of immiscible poly(n butyl acrylate) (block A) and gradient copolymers of methyl methacrylate (MMA) and n butyl acrylate (n BA) (block M/A) were investigated by means of their heat capacity, Cp, as a function of the composition of the blocks M/A and temperature. In all copolymers studied, both blocks are represented by their...

متن کامل

Fabrication and Characterization of Proton Conductive Membranes Based on Poly(methyl methacrylate-co-maleic anhydride)

In this study, proton conductive composite membranes were produced by using a poly(methylmethacrylate-co-maleic anhydride) (P(MMA-co-MAH)) copolymer and phosphotungstic Acid (PWA) as an additive of the proton conductive agent. P(MMA/MAH) 70/30, 50/50, and 30/70 were synthesized using a free radical polymerization reaction. PWA with a concentration of 2% was added to...

متن کامل

Cisplatin delivery from poly(acrylic acid-co-methyl methacrylate) microparticles.

To develop a platform for tumor chemotherapy, poly(acrylic acid-co-methyl methacrylate) microparticles have been synthesized. Carboxylate containing monomers were included to complex therapeutic agents, specifically cisplatin. Microparticles were prepared by free radical emulsion polymerization in aqueous media. Particle diameter, zeta-potential, in vitro cytotoxicity, and in vivo acute toxicit...

متن کامل

Electrospinning of Poly (mma-co-maa) Copolymers and Their Layered Silicate Nanocomposites for Improved Thermal Properties

Copolymers consisting of methyl methacrylate (MMA) and methacrylic acid (MAA) and their layered silicate nanocomposites were electrospun to form fibers with diameters in the sub-micron range. The presence of MAA increased the glass transition temperature and thermal stability of the copolymers through formation of anhydrides upon heating. Dispersion of layered silicates within the nanocomposite...

متن کامل

Solubility and diffusivity of solvents and nonsolvents in poly(methyl methacrylate co butyl methacrylate)

In this study, thermodynamic properties, namely retention volume, infinitely dilute weight fraction activity coefficient, Flory–Huggins interaction parameter, solubility parameter of the polymer, partition coefficient and diffusion coefficients of the various solvents in poly(methyl methacrylate co butyl methacrylate) (PMMA co BMA) at infinite dilution of the solvent have been determined by inv...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Applied Sciences

سال: 2002

ISSN: 1812-5654

DOI: 10.3923/jas.2002.400.404