Directional Solidification Microstructure Control in CM247LC Superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Directional Solidification Microstructure of a Ni-Based Superalloy: Influence of a Weak Transverse Magnetic Field

A Ni-based superalloy CMSX-6 was directionally solidified at various drawing speeds (5–20 μm·s−1) and diameters (4 mm, 12 mm) under a 0.5 T weak transverse magnetic field. The results show that the application of a weak transverse magnetic field significantly modified the solidification microstructure. It was found that if the drawing speed was lower than 10 μm·s−1, the magnetic field caused ex...

متن کامل

Numerical Simulation and Optimization of Directional Solidification Process of Single Crystal Superalloy Casting

The rapid development of numerical modeling techniques has led to more accurate results in modeling metal solidification processes. In this study, the cellular automaton-finite difference (CA-FD) method was used to simulate the directional solidification (DS) process of single crystal (SX) superalloy blade samples. Experiments were carried out to validate the simulation results. Meanwhile, an i...

متن کامل

Solidification microstructure development

In the present article, evolution of microstructure during solidification, as a function of various parameters, is discussed. Macrosegregation is described as being due to insufficient diffusivity of solute in the solid. Pattern formation is discussed in the light of instabilities at the solidification growth front. An overview of the scaling relations for various microstructures is given. Meta...

متن کامل

Dynamical microstructure formation in 3D directional solidification of transparent model alloys: in situ characterization in DECLIC Directional Solidification Insert under diffusion transport in microgravity

To clarify and characterize the fundamental physical mechanisms active in the dynamical formation of three-dimensional (3D) arrays of cells and dendrites under diffusive growth conditions, in situ monitoring of series of experiments on transparent model alloy succinonitrile – 0.24 wt% camphor was carried out under low gravity in the DECLIC Directional Solidification Insert on-board the Internat...

متن کامل

Cellular instabilities in directional solidification

2014 We have studied the morphology of the solid-liquid interface during the directional solidification of thin (5-150 03BCm) samples of a dilute binary mixture (CBr4/~ 0.1 % Br2) . Above a critical pulling speed, for a given temperature gradient and solute concentration, the interface, initially planar, breaks down into a periodic cellular pattern. The bifurcation from a planar to a cellular s...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Today: Proceedings

سال: 2014

ISSN: 2214-7853

DOI: 10.1016/j.matpr.2014.09.002