Dissimilar Friction Stir Welding of Ni-Base Superalloy with Al Alloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Analysis and Comparison of Friction Stir Welding and Laser Assisted Friction Stir Welding of Aluminum Alloy

Friction Stir Welding (FSW) is a solid-state joining process; i.e., no melting occurs. The welding process is promoted by the rotation and translation of an axis-symmetric non-consumable tool along the weld centerline. Thus, the FSW process is performed at much lower temperatures than conventional fusion welding, nevertheless it has some disadvantages. Laser Assisted Friction Stir Welding (LAFS...

متن کامل

Friction stir welding of dissimilar alloys – a perspective

Friction stir welding does not involve bulk melting of the components that are joined. This has inspired attempts to exploit it for joining materials which differ in properties, chemical composition or structure, and where fusion can lead to detrimental reactions. The purpose of this special issue of Science and Technology of Welding and Joining was to assess the status of friction stir welding...

متن کامل

Forming and Properties of Friction Stir Welding Process for Dissimilar Mg Alloy

For hot extrusions of magnesium alloy sheets, Dissimilar AZ80 and AZ31 were used, in which AZ80 was placed on advancing side and AZ31 on retreating side, using friction stir butt welding with different process parameters. Some defect-free welded joints with good weld surfaces could be obtained with some suitable welding conditions. The maximum tensile strength of welded joint which is 225.5 MPa...

متن کامل

Liquation Cracking of Dissimilar Aluminum Alloys during Friction Stir Welding

A liquation cracking mechanism of dissimilar Al alloys during the friction stir welding (FSW) is suggested in this study. To identify the mechanism, the precipitates were analyzed and Al-Mg-Cu phase diagrams were calculated. Electron backscattering diffraction (EBSD) analysis and electron probe microanalysis (EPMA) were also conducted. In the same manner as constitutional liquation, at high hea...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A

سال: 2011

ISSN: 0387-5008,1884-8338

DOI: 10.1299/kikaia.77.708