Dynamic nanoindentation testing: is there an influence on a material’s hardness?

Modern nanoindentation devices are capable of dynamic experimentations, which allow us to exploit instrumented hardness tests extensively. Beside the assets of recording mechanical properties continuously over displacement, there are ongoing debates whether the superimposed force alters the material's hardness. We will show for a broad range of materials that significant hardness differences ar...

متن کامل

Nanoindentation studies of materials

have recognized that surface contacts between materials are highly dependent on their mechanical properties1,2. Many different indentation and impression tests have been developed in an effort to measure such mechanical properties from a contact of known geometry. In the past two decades, however, a veritable revolution has occurred in indentation testing, owing to the development of new sensor...

متن کامل

Why Believe That There Is a God?

This article presents an argument for the existence of God, showing that the evident phenomena are best explained by supposing that a God causes them. The argument is based on the inductive force of four very evident general phenomena: that there is a physical Universe; that it is governed by very simple natural laws; that those laws are such as to lead to the existence of human bodies; and tha...

متن کامل

Vitamin D: Is There a New Era?

  Background: In recent decades, much interest has been focused on investigating new roles of vitamin D in human body beyond the mineral-ion homeostasis. Methods: By searching medical databases such as PubMed, over 16000 articles were found which have been published since 2000 on novel aspects of vitamin D in health and diseases. Results: Of great interest was the effects of vitamin D on ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Research Letters

سال: 2017

ISSN: 2166-3831

DOI: 10.1080/21663831.2017.1331384