Effect of Equal Channel Angular Pressing on the Pitting Corrosion Resistance of Aluminum-Copper Alloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Equal Channel Angular Pressing and Annealing Treatment on the Evolution of Microstructure in AlMg0.7Si Aluminum Alloy

In this research, samples of AlMg0.7Si aluminum alloy are deformed up to three passes using equal channel angular pressing (ECAP). Formation of a sub-micron structure after three passes of ECAP is demonstrated. Microstructural stability of the samples is investigated at temperatures of 300-500 °C. At 300 °C, fine recrystallized structure forms after 10 min which remains stable when the ...

متن کامل

Plastic deformation of 7075 Aluminum Alloy using Integrated Extrusion-Equal Channel Angular Pressing

Grain refinement improves the mechanical properties and formability of metals and alloys. So far, several different grain refinement methods have been proposed and studied. Severe plastic deformation is one of the most promising and efficient methods. Therefore, in the present study the possibility of imposing a two-step severe plastic deformation (Extrusion and Equal channel angular pressing) ...

متن کامل

Re-strengthening in AA6063 Alloy During Equal Channel Angular Pressing

Equal channel angular pressing (ECAP) is carried out using two different configurations for the exit channel of the ECAP die, i.e., relieved and choked, with angles of 0.2 °. It is found that using a die with relieved exit channel, the sample was extruded for 6 passes with no surface cracks and an average cell size of 727 nm and a fraction of high angle grain boundaries of 54 % were achieved. M...

متن کامل

Size effect in equal channel angular pressing (ECAP) process

The influence of the sample size (diameter while keeping the length constant) in equal channel angular pressing (ECAP) of pure aluminum is examined using finite element method (FEM) and experiment. Different sized aluminum rods were processed via ECAP and the effect of sample size on the strain homogeneity, process load, and the ratio of the friction to the total force were evaluated. The resul...

متن کامل

Experimental Investigation of Thermal Conductivity of Aluminum Alloy 3003 Produced by Equal Channel Angular Rolling Process

Equal channel angular rolling (ECAR) process is one of the methods that have been used to make ultra-fine materials by imposing severe plastic deformation. After repeating the process several times, a large effective strain is applied to the sample that can cause decreasing the grain size and improving the mechanical and physical properties of the metal. In this study, thermal conductivity of t...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of The Surface Finishing Society of Japan

سال: 2010

ISSN: 0915-1869

DOI: 10.4139/sfj.61.50