Effect of Metallurgical Factors of Low Carbon Steel Sheets on Stress Corrosion Cracking in Methanol Solution
نویسندگان
چکیده
منابع مشابه
An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution
The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...
متن کاملCorrosion Inhibition Effect of Ester Containing Cationic Gemini Surfactants on Low Carbon Steel
α, ω-alkane-bis(N-myristoyloxyethyl-N, N-dimethyl)-diammonium bromide were synthesized<span style="font-size: 10.0pt; line-height...
متن کاملthe washback effect of discretepoint vs. integrative tests on the retention of content in knowledge tests
در این پایان نامه تاثیر دو نوع تست جزیی نگر و کلی نگر بر به یادسپاری محتوا ارزیابی شده که نتایج نشان دهندهکارایی تستهای کلی نگر بیشتر از سایر آزمونها است
15 صفحه اولEffect of Dates Extracts as Environmentally Friendly Corrosion Inhibitor for Carbon Steel in 1M HCl Solution
Inhibitory effect of extracts from three date varieties namely khalt (kha), Lassiane (La) and Tadmamt (Td)), and the mixture of date varieties as environmentally friendly corrosion inhibitor for carbon steel in 1M HCl is studied by means of electrochemical tests such as electrochemical impedance spectroscopy (EIS), and Tafel polarization. It's been obtained that in 1.0 M HCl solution the date e...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Transactions of the Iron and Steel Institute of Japan
سال: 1978
ISSN: 0021-1583,1881-1183
DOI: 10.2355/isijinternational1966.18.554