Effect of Pre-Post TIG Welding Heat Treatment on Cast NI Superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

the effect of heat treatment on the microstructure of cast ni-based in100 superalloy

the purpose of this study was to investigate the effect of heat treatment including solution treatment and aging on the microstructure of cast nickel-based in100 superalloy including size, volume fraction and morphology of primary γ' and different kinds of carbides. for this purpose, different solution heat treatment cycles and a constant aging cycle were implemented on cast ingot samples and t...

متن کامل

The Effect of High Temperature Exposure on Dendritic Segregation in a Conventionally Cast Ni Based Superalloy

Dendritic segregation in conventionally cast, commercially heat treated and exposed MarM002 turbine blades has been investigated using scanning electron microscopy (SEM) and energy dispersive X-ray analysis (EDS). During casting Cr, Co and W segregate to the dendrites and Hf, Ti and Ta segregate to the eutectics. As a result of the dissolution of γ' precipitates in the dendrites and coarsening ...

متن کامل

Comparative Study of Tig and Smaw Root Welding Passes on Ductile Iron Cast Weldability

J. Cárcel-Carrasco; M. Pascual; M. Pérez-Puig; F. Segovia. ITM-Universitat Politècnica de València (Spain). Camino de vera s/n, 46022 Valencia (Spain). Corresponding author, Email: [email protected] This work compares the weldability of ductile iron when: (I) a root weld is applied with a tungsten inert gas (TIG) process using an Inconel 625 source rod and filler welds are subsequently applie...

متن کامل

Effect of pre-exposure on crack initiation life of a directionally solidified Ni-base superalloy

Article history: Received 6 February 2008 Received in revised form 1 July 2008 Accepted 24 July 2008 Available online 5 August 2008

متن کامل

Tig Welding Process Pdf

Tungsten inert gas (TIG) welding, also called as gas tungsten welding 1. (a) Schematic of TIG welding Process (b) Variety of tungsten electrodes. The activated TIG (ATIG) welding process mainly focuses on increasing the depth of penetration and the reduction in the width of weld bead has not been paid. Tungsten inert gas welding, TIG is widely applied in manufacturing process for different The ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Annals of Dunarea de Jos University of Galati Fascicle XII Welding Equipment and Technology

سال: 2020

ISSN: 1221-4639,2668-6163

DOI: 10.35219/awet.2020.05