Effects of NaCl concentration on galvanic corrosion behavior of aluminum alloy A5052/carbon steel SS400 couple

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A Galvanic Corrosion Approach to Investigating Chromate Effects on Aluminum Alloy 2024-T3

The effects of chromate treatment on the corrosion of an aluminum/copper aircraft alloy were examined with a galvanic corrosion apparatus composed of two electrodes and a zero resistance ammeter. Combinations of pure Al, pure Cu, and AA2024-T3 electrodes were immersed in 0.1 M NaCl solution, which was saturated with air, O2 , or argon. Selection of electrode material or differential aeration re...

متن کامل

Corrosion Behavior of Tin-Plated Carbon Steel and Aluminum in NaCl Solutions Using Electrochemical Impedance Spectroscopy

The corrosion behavior of both tin-plated carbon steel and aluminum (Al 1100) in NaCl solutions were studied using electrochemical impedance spectroscopy (EIS). The study objectives were to compare their corrosion behavior in concentrated brine solution, establish the equivalent electrical circuit diagrams of their corrosion phenomena, and consequently develop steady-state corrosion models for ...

متن کامل

Investigation of Corrosion Behavior and Galvanic Corrosion Simulation of Super Duplex Stainless Steel UNS S32750 Weld Zone

Galvanic corrosion is an ever-present problem in all different environments, particularly in tanks. The goal of this project is to develop a finite element model that can be used with experimental data to characterize the corrosion of a galvanic weldments couple in an electrolyte. In this study sample are welded by gas tungsten arc welding and friction stir welding. According to ASTM G8, Evalua...

متن کامل

Investigation of Corrosion Behavior and Galvanic Corrosion Simulation of Super Duplex Stainless Steel UNS S32750 Weld Zone

Galvanic corrosion is an ever-present problem in all different environments, particularly in tanks. The goal of this project is to develop a finite element model that can be used with experimental data to characterize the corrosion of a galvanic weldments couple in an electrolyte. In this study sample are welded by gas tungsten arc welding and friction stir welding. According to ASTM G8, Evalua...

متن کامل

Corrosion behavior of dissimilar welded joint between Inconel 617 alloy and A387-Gr.11 low-alloy steel

In this study, Inconel 617 alloy was welded to A387-Gr.11 low-alloy steel using ER309L filler metal via gas tungsten arc welding (GTAW). First, the corrosion behavior of Inconel 617, A387-Gr, and the weld metal was evaluated by the Tafel polarization test and electrochemical impedance spectroscopy (EIS) in acidic (H2SO4), neutral (NaCl), and combined (H2SO4 + NaCl) solution at ambient temperatu...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Japan Institute of Light Metals

سال: 2021

ISSN: 0451-5994,1880-8018

DOI: 10.2464/jilm.71.89