Elucidating the growth mechanism of ZnO films by atomic layer deposition with oxygen gas <i>via</i> isotopic tracking

نویسندگان

چکیده

The growth process of zinc oxide (ZnO) thin films by atomic layer deposition (ALD) accompanied the presence oxygen gas pulsing is investigated means isotopic tracking 18O from water precursor and 16O gas.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effects of Al Doping on the Properties of ZnO Thin Films Deposited by Atomic Layer Deposition

The tuning of structural, optical, and electrical properties of Al-doped ZnO films deposited by atomic layer deposition technique is reported in this work. With the increasing Al doping level, the evolution from (002) to (100) diffraction peaks indicates the change in growth mode of ZnO films. Spectroscopic ellipsometry has been applied to study the thickness, optical constants, and band gap of...

متن کامل

On the environmental stability of ZnO thin films by spatial atomic layer deposition

• A submitted manuscript is the author's version of the article upon submission and before peer-review. There can be important differences between the submitted version and the official published version of record. People interested in the research are advised to contact the author for the final version of the publication, or visit the DOI to the publisher's website. • The final author version ...

متن کامل

Effects of doping and annealing on properties of ZnO films grown by atomic layer deposition

Undoped and Al-doped ZnO films were synthesized by atomic layer deposition at 150°C and then annealed at 350°C in different atmospheres. Effects of doping and annealing on the film growth mode and properties were investigated. The undoped film has strong UV emission and weak Zn interstitial emission. Annealing introduces O vacancies, decreases Zn interstitials, and results in weakening and blue...

متن کامل

Atomic layer deposition of Zn(O,S) thin films with tunable electrical properties by oxygen annealing

Zinc oxysulfide, Zn(O,S), films grown by atomic layer deposition were annealed in oxygen to adjust the carrier concentration. The electron carrier concentration of Zn(O,S) can be reduced by several orders of magnitude from 10 to 10 cm 3 by post-deposition annealing in oxygen at temperatures from 200 C to 290 C. In the case of Zn(O,S) with S/Zn1⁄4 0.37, despite the considerable change in the ele...

متن کامل

Structural, electrical, and optical properties of Ti-doped ZnO films fabricated by atomic layer deposition

High-quality Ti-doped ZnO films were grown on Si, thermally grown SiO2, and quartz substrates by atomic layer deposition (ALD) at 200°C with various Ti doping concentrations. Titanium isopropoxide, diethyl zinc, and deionized water were sources for Ti, Zn, and O, respectively. The Ti doping was then achieved by growing ZnO and TiO2 alternately. A hampered growth mode of ZnO on TiO2 layer was co...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Materials Chemistry C

سال: 2021

ISSN: ['2050-7526', '2050-7534']

DOI: https://doi.org/10.1039/d0tc05439a