Estimation of Creep Constitutive Law for Cr-Mo-V Material in Turbine Rotor Using Indentation Creep Test
نویسندگان
چکیده
منابع مشابه
Indentation vs. Uniaxial Power-law Creep of Sn-based Solder Material: A Numerical Assessment
It is crucial to understand the creep behavior of Pb-free solder alloys in electronic packaging. Typical service environments are between 298 and 373K. The thermal mismatch induced stresses acting on solder joints result in extensive rate-dependent plastic deformation. The solder alloy is potentially the weakest component in the electronic package because normal operating temperatures are alrea...
متن کاملA Review of Creep Deformation and Rupture Mechanisms of Cr-Mo Alloy for the Development of Creep Damage Constitutive Equations under Lower Stress
This paper presents a review of creep deformation and rupture mechanisms of low Cr-Mo alloy for the development of its creep damage constitutive equations under lower stress. The most popular Kachanov-Robatnov-Hayhurst (KRH) formulation was not necessarily developed and calibrated for low stress and cannot depict the creep strain accurately under multi-axial state of stress due to the three-dim...
متن کاملThe development of creep damage constitutive equations for low Cr-Mo alloy steel and its weldment at low stress
The ultimate objective of this research project is to develop creep damage constitutive equations for low Cr-Mo alloy and its weldment under low stress (0.2-0.4 yield stress, ��). This paper summarizes a critical analysis on the cavity nucleation and growth and the deformation mechanisms and creep damage evolution characteristics at low stress with temperature ranging from 450 °C to 650 °C, in ...
متن کاملA New Method for Estimation of Creep of Concrete Using Short-TermTests under Higher Temperature
In the Present study, attempt will be made to propose a new method for prediction of long-term essential creep of concrete utilizing some short-term creep tests under high temperature. To do so, regarding the similarities between essential creep of concrete and creep in viscoelastic materials, the time–temperature equivalence relation in viscoelastic materials is evaluated for concrete. This re...
متن کاملAnalysis on Pseudo-steady Indentation Creep
Theoretical analysis and finite element (FE) simulation have been carried out for a constant specific load rate (CSLR) indentation creep test. Analytical results indicate that both the representative stress and the indentation strain rate become constant after a transient period. Moreover, the FE simulation reveals that both the contours of equivalent stress and equivalent plastic strain rate u...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 2004
ISSN: 1880-7488,0514-5163