Evaluations of KISCC, KIH and subcritical crack growth rate by holding-load and fractography test.
نویسندگان
چکیده
منابع مشابه
Subcritical crack growth law and its consequences
For brittle failures, the probability distribution of structural strength and lifetime are known to be Weibullian, in which case the knowledge of the mean and standard deviation suffices to determine the loading or time corresponding to a tolerable failure probability such as 10−6. Unfortunately, this is not so for quasibrittle structures, characterized by material inhomogeneities that are not ...
متن کاملThe link of arms holding infant and growth rate
Introduction: In the first 6 months of life, infant growth had maximum of its speed but abnormality growth may reflect on a chronic disease, inadequate nutrition or may be depend on another complications such as dietary, psychosocial development Objective: The goal of this study was to investigate relationship of In-Arms holding a baby during breast feeding and growth rate in Kashan health c...
متن کاملconstruction and validation of the translation teacher competency test and the scale of students’ perceptions of translation teachers
the major purpose of this study was to develop the translation teacher competency test (ttct) and examine its construct and predictive validity. the present study was conducted in two phases: a qualitative phase as well as a quantitative phase. in the first phase of the study, the author attempted to find out the major areas of competency required for an academic translation teacher. the second...
Subcritical Crack Growth and Its Relation to Predictive Analysis
This talk will discuss the relationships between subcritical crack growth and the nature of the loading, the environment under which the loading takes place and the type of material tested, and how this data is used in predictive analysis. Loading conditions will include sustained loading as well as constant and variable amplitude cyclic loading. The environments will include vacuum as a baseli...
متن کاملexploring motivation and english test preparation strategies of iranian pre-university candidates during and at the end of test preparation period for konkur examination
the current study aimed at investigating the relationship between motivation and test preparation strategies (tpss) used by iranian pre-university students in their preparation period for the university entrance exam (uee). due to the importance of uee in iran, this study also attempted to show its impact on these two important variables. to this end, 100 pre-university students in an iranian p...
ذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 1987
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.36.267