Evolution Laws of 7B04 Aluminum Alloys Pitting Corrosion Topography Characteristics and Size Parameters
نویسندگان
چکیده
منابع مشابه
Characterization of pitting corrosion in aluminum films by light scattering
We report a detailed study of the morphology of pits formed by corrosion of aluminum thin films using an in-plane light scattering technique. We show that the corrosion front of the Al thin film can be treated as a quasi-two-level random rough surface. Based on an elastic diffraction theory, we are able to determine the average depth, the area, and the density of pits, as well as the fractal di...
متن کاملStudy of Copper Bearing Alloys Corrosion Characteristics
This paper addresses investigation of the corrosion behavior of copper bearing anodes with high nickel content. Anodes are produced from different solid wastes formed during the copper or nickel row materials treatment. Nickel content in anode samples had values up to 10 mas %. The content of tin, lead and antimony was up to 1 % for each of elements. Sulphuric acid solution, concentration of 17...
متن کاملTHE ROLE OF ALKALINE CLEANING SOLUTIONS AND CL-CONTAINING LUBRICANTS ON PITTING CORROSION IN NiTi ALLOYS
Alkaline cleaning agents are found to react with remnant manufacturing lubricants trapped in surface defects of a NiTi alloy to form Cl-based salts. These sub-surface “reservoirs” may act as nucleation sites for pitting corrosion either latent under ambient conditions, or on exposure to a limited range of high temperatures used to impart pseudoelastic properties in these alloys as part of norma...
متن کاملPitting Corrosion of Heat-treatable Aluminium Alloys and Welds: a Reveiw
This review attempts to present the current understanding of the mechanism of pitting corrosion of heat treatable aluminium alloys and their welds. The role of alloying elements and intermetallic phases on the corrosion behavior of these alloys has been discussed. Pitting mechanism of aluminiumcopper alloys is specifically discussed. Finally effect of welding on the pitting corrosion of these a...
متن کاملActivation of Aluminum as an Effective Reducing Agent by Pitting Corrosion for Wet-chemical Synthesis
Metallic aluminum (Al) is of interest as a reducing agent because of its low standard reduction potential. However, its surface is invariably covered with a dense aluminum oxide film, which prevents its effective use as a reducing agent in wet-chemical synthesis. Pitting corrosion, known as an undesired reaction destroying Al and is enhanced by anions such as F⁻, Cl⁻, and Br⁻ in aqueous solutio...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: DEStech Transactions on Computer Science and Engineering
سال: 2019
ISSN: 2475-8841
DOI: 10.12783/dtcse/ica2019/30747