Evolution of microstructure and twin density during thermomechanical processing in a γ-γ’ nickel-based superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evolution of the Annealing Twin Density during -Supersolvus Grain Growth in the Nickel-Based Superalloy InconelTM 718

Grain growth experiments were performed on InconelTM 718 to investigate the possible correlation of the annealing twin density with grain size and with annealing temperature. Those experiments were conducted at different temperatures in the supersolvus domain and under such conditions that only capillarity forces were involved in the grain boundary migration process. In the investigated range, ...

متن کامل

Influence of the initial cooling rate from γ’ supersolvus temperatures on microstructure and phase compositions in a nickel superalloy

Different cooling paths from a supersolvus temperature have been applied to FGH96, a polycrystalline nickel base superalloy for turbine disc applications, in order to simulate the different microstructures that exist through the thickness of a disc following an industrial heat treatment. Secondary and tertiary γ’ precipitate size distributions and morphology have been analysed and compared for ...

متن کامل

Flow Stress Modeling in a γ-γ/ Cobalt Base Superalloy by Using the Hyperbolic Sine Equation and ANN Method

The new class of wrought γ-γ/ Co-base superalloys, which are based on Co-Al-W system,  was developed by conventional hot working routes with a high volume fraction of γ/ precipitates and good mechanical properties. The aim of the present study was to predict the flow stress and hot deformation modeling of a novel γ-γ/ Co-base superalloy. The hot compression test...

متن کامل

Effect of Thermomechanical Processing on the Microstructure and Mechanical Properties of a Duplex Stainless Steel

Duplex stainless steels (DSSS) have a microstructure composed of ferrite and austenite phases that gives them a very good combination of mechanical and corrosion properties. These steels are desirable for many applications in the chemical and petrochemical industries. In the present study, a type of stainless steel was cast, solution annealed at 1200°C for 60 min and then quenched in water. Ini...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Materialia

سال: 2012

ISSN: 1359-6454

DOI: 10.1016/j.actamat.2012.06.028