Fractographic Analysis of Co-P-SiC Electrocomposite Coatings by Stereoscopic Reconstruction

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fractographic Analysis of Co-P-SiC Electrocomposite Coatings by Stereoscopic Reconstruction

Electrolytic Hard Chrome (EHC) coatings are widely employed to improve the surface performance of engineering components. The superior wear and corrosion resistance, combined with the processing advantage of being able to coat surfaces with complex geometries, makes EHC a preferred choice for coating critical components like aircraft landing gear, hydraulic actuator cylinders, etc. There are, h...

متن کامل

ELECTRODEPOSITION AND CHARACTERIZATION OF Ni - Co - P - BN DISPERSION COATINGS

Functional plating such as alloys or dispersion coatings have been widely used in metal finishing industry. In general, dispersion coatings are deposited from plating baths containing suspended particles such as metal oxides, carbides, metals or organic materials,(l-3) Codeposited particles in the dispersion coatings have the remarkable influence on the properties of the deposits depending on t...

متن کامل

Stereoscopic liver surface reconstruction

The paper presents a practical approach to measuring liver motion, both respiratory and laparoscopic, with a tool guided in the operating room. The presented method is based on standard operating room equipment, i.e. rigid laparoscopic cameras and a single incision laparoscopic surgery trocar. The triangulation algorithm is used and stereo correspondence points are marked manually by two indepe...

متن کامل

DEVELOPMENT OF CVD MULLITE COATINGS FOR SiC FIBERS

1.0 Introduction 2.0 Experimental details 2.1 CVD process 2.2 Oxidation Testing 2.3 Cyclic Oxidation Testing 2.4 Corrosion Testing 2.5 Tensile Testing 3.0 Results and discussion 3.1 3.2 3.3 3.4 3.5 3.6 Effect of system parameters 3.1.1 System pressure 3.1.2 Input gas velocity 3.1.3 A1/Si molar ratio Structure of mullite coating Oxidation Testing Cyclic Oxidation Hot Corrosion Tensile Strength 4...

متن کامل

Preparation of β-SiC Coatings Using 1,2-Dimethyldisilane as Precursor

A cold-wall upstream reactor was designed to study the deposition of P-Sic layers on WC-Co hard metal substrates. Experiments demonstrated that P-Sic coatings can be easily deposited on inductively heated substrates at temperatures between 1000-1400°C by thermal decomposition of 1,2-dimethyldisilane under normal pressure conditions. It was shown that this silicon compound is an advanced precurs...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Microscopy and Microanalysis

سال: 2014

ISSN: 1431-9276,1435-8115

DOI: 10.1017/s1431927614011155