Fractographic Analysis of Fracture Surface of Sintered Silicon Nitride Fractured under Static or Cyclic Load.

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Structural and Electrical Characterization of Sintered Silicon Nitride Ceramic

The electrical conduction phenomena, dielectric response and microstructure have been discussed in sintered silicon nitride ceramics at different temperature and frequencies. Microstructure and phase of the sintered samples was investigated by Scanning Electron Microscope (SEM) and X-ray diffractometer (XRD). The electrical conductivity, dielectric constant and dielectric loss increases exponen...

متن کامل

Microstructure of Spark Plasma-Sintered Silicon Nitride Ceramics

The microstructure and phase composition of the high-content Al2O3-Y2O3-doped spark plasma-sintered silicon nitride were investigated. Fully dense silicon nitride ceramics with a typical α-Si3N4 equiaxed structure with average grain size from 200 to 530 nm, high elastic modulus of 288 GPa, and high hardness of 2038 HV were spark plasma sintered (SPSed) at 1550 °C. Silicon nitride with elongated...

متن کامل

Interfacial structure in silicon nitride sintered with lanthanide oxide

Three independent research groups present a comparison of their structural analyses of prismatic interfaces in silicon nitride densified with the aid of lanthanide oxide Ln2O3. All three groups obtained scanning transmission electron microscope images which clearly reveal the presence of well-defined Ln segregation sites at the interfaces, and, moreover, reveal that these segregation sites are ...

متن کامل

Effect of Stress Pattern on Fatigue Strength of Sintered Silicon Nitride by

It is difficult to conduct cyclic tensile fatigue tests for fine ceramics because of its high brittleness, and a little eccentricity of loading axis and gripping device gives inaccurate strength data. So, a major part of cyclic fatigue tests have been carried out under bending load conditions, for the allowance of misalignment of loading axis is generous to some extent in the case of bending fa...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1991

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.40.695