Fractographic analysis of the aluminum matrix composite prepared by accumulative roll bonding

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Accumulative Roll Bonding of Aluminum/Stainless Steel Sheets

An Al/Stainless Steel/Al lamellar composite was produced by roll bonding of the starting sheets at 400 °C. Afterward, the roll bonded sheet was cut in half and the accumulative roll bonding (ARB) process at room temperature was applied seven times. As a result, the central steel layer fractured and distributed in the Al matrix among different layers introduced by the repetition of roll bonding ...

متن کامل

A Comparative Corrosion Study of Al/Al2O3-SiC Hybrid Composite Fabricated by Accumulative Roll Bonding (ARB)

In this study, the Al/Al2O3-SiC hybrid composite was produced by accumulative roll bonding (ARB). In the first and the second cycles, the particles were uniformly poured between the Al strips during each ARB cycle. In the subsequent cycles, ARB was repeated up to six cycles without adding the particles between the layers. After the total eight cycles, the particles were distributed uniformly wi...

متن کامل

Computational evaluation of the homogeneity of composites processed by accumulative roll bonding (ARB)

A new computational method based on MATLAB was used to study the effect of different parameters on the homogeneity of composites produced by a severe plastic deformation technique known as accumulative roll bonding. For a higher number of passes, the degree of particle agglomeration and clustering decreased, and an appreciable homogeneity was obtained in both longitudinal and transverse directi...

متن کامل

Cyclic Deformation of Ultra-Fine Grained Commercial Purity Aluminum Processed by Accumulative Roll-Bonding

Accumulative Roll-Bonding (ARB) is one of the more recently developed techniques capable of producing bulk ultra-fine grained (ufg) metals. There are still many aspects of the behavior of ufg metals that lacks an in-depth understanding, such as a generalized view of the factors that govern the cyclic deformation mechanism(s). This study aims to advance the understanding of the cyclic deformatio...

متن کامل

Fabrication of nanostructured aluminum sheets using four-layer accumulative roll bonding

In this paper, an extended accumulative roll bonding (ARB) technique, called the 'Four-Layer Accumulative Roll Bonding (FL-ARB)' technique, is presented for the first time. This technique has been employed to produce ultrafine-grained commercial pure aluminum sheets with success. After three FL-ARB passes, the grain size of pure aluminum was seen to reduce to 380 nm. The bonding strength of the...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Engineering

سال: 2020

ISSN: 2217-8961

DOI: 10.30544/569