Fractured Metallic Tracheostomy Tube: Report of a Fractographic Study
نویسندگان
چکیده
منابع مشابه
Fractured metallic tracheostomy tube: A rare complication of tracheostomy
Although tracheostomy is a well-accepted procedure for airway management, some early and late complications may occur. Fracture of the tracheostomy tube (TT) is a rare complication, particularly in a patient with long-term use. Herein we report a case of fractured metallic TT migrating into the tracheobronchial tree. Rigid bronchoscopy was performed through the tracheostomy stoma and the fractu...
متن کاملFractured metallic tracheostomy tube in a child: a case report and review of the literature
INTRODUCTION Tracheostomy is a common airway procedure for life support. The fracture of the tracheostomy tube is a rare complication. We report a case of a 14-year-old boy whose fractured stainless steel tracheostomy tube dislodged into the tracheobronchial tree. We include a literature review and proposed recommendations for tracheostomy care. CASE PRESENTATION A 14-year-old Thai boy who ha...
متن کاملA Broken Metallic Tracheostomy Tube
Tracheostomy is an upper airway bypass which is life saving in certain occasions. However, there are several early and late complications. One of these rare mishaps is the broken cannula, few cases of which has been reported so far. Herein we are reporting a rare case of broken tube as a late complication of indwelling tracheostomy tube. A 52 year old woman with moderate respiratory distress wa...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Health Science and Medical Research
سال: 2021
ISSN: 2630-0559,2586-9981
DOI: 10.31584/jhsmr.2021789