Gigacycle Fatigue Behaviour and Fractography of Extruded AZ80 Magnesium Alloy

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue behaviour and fractography of extruded AZ80 magnesium alloys in very high cycle regime

In order to investigate the fatigue properties of extruded magnesium alloy in very high-cycle regime, rotary bending fatigue test was performed in ambient atmosphere at room temperature using the hourglass shaped specimens of AZ80 alloys extruded (Fspecimen) and treated by an artificial aging after extrusion (T5-specimen). From the experimental results, both specimens show a clear step-wise S-N...

متن کامل

Kinetics of SIMA AZ80 Magnesium Alloy

Semi-solid feedstock of AZ80 magnesium alloy modified by [trace] rare-earth Y element 10 (0, 0.2, 0.4, 0.8 wt.%) were fabricated by [strain-induced melting activation] (SIMA) in the form of 11 extrusion and partial remelting. The effect of Y addition on the microstructure evolution of [the] 12 extruded and [isothermally heat] treated alloy was observed by [using an] optical microscope (OM), 13 ...

متن کامل

Grain Refinement and Enhancement of Mechanical Properties of Hot Extruded Rare-Earth Containing Magnesium Alloy

The effects of rare earth addition and hot extrusion process on the grain refinement of magnesium alloy were studied. The as-cast Mg-6Al-1Zn (AZ61) alloy had the average grain size of ~ 64 µm and its microstructure consisted of α-Mg and Mg17Al12 phase. By partial substitution of Al with Gd to reach Mg-4.8Gd-1.2Al-1Zn alloy, it was observed that the Mg17Al12 phase disappeared and two new interme...

متن کامل

High Frequency Fatigue Test of in 718 Alloy – Microstructure and Fractography Evaluation

J. Belan, Faculty of Mechanical Engineering, University of Žilina, Žilina, Slovak Republic INCONEL alloy 718 is a high-strength; corrosion-resistant nickel chromium material used at -253 °C to 705 °C for production of heat resistant parts of aero jet engine mostly. The fatigue test provided on this kind materials were done via low frequency loading up to this time. Nowadays, needs of results at...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Transactions of the Japan Society of Mechanical Engineers Series A

سال: 2009

ISSN: 0387-5008,1884-8338

DOI: 10.1299/kikaia.75.733