Investigation of the Heat Treatment Effect on Microstructures and Phases of Inconel 713C Superalloy
The application of Inconel 713C is very vast in different industries such as in automobiles, aircrafts, boilers and turbines. In this paper, Inconel 713C specimens were solutionized at 1000 and 1200 °C for 1 hours in order to study changes in phases and the structure of alloy to modify the γ' phase. The optical and the scanning electron microscopy were used to investigate the structure and the ...
متن کاملEffects of Ageing and Forging on Short-term Creep Behaviors of Inconel-713C Superalloy at 850 °C
In this paper, the short-term creep behavior of the Inconel-713C superalloy after different pre-treatments including the ageing and forging processes has been studied at 850 °C. The ageing heat treatment was heating at 930 °C for 16 hours without solutioning process. The optical microscopy (OM) and the scanning electron microscopy (SEM) techniques were applied for microstructural evaluations. T...
متن کاملParametric optimization of powder mixed electrical discharge machining for nickel-based superalloy inconel-800 using response surface methodology
Background: Electrical Discharge Machining (EDM) is a well-established non-conventional machining process for the machining of electrically conductive and difficult-to-machine materials. But its applications are limited because of the slow machining rate and poor surface finish. Powder mixed EDM (PMEDM) is unitary of the recent progresses in the EDM process in which powder particles mixed in th...
متن کاملSelective Growth of Low Stored Energy Grains During δ Sub-solvus Annealing in the Inconel 718 Nickel-Based Superalloy
The microstructure stability during d sub-solvus annealing in Inconel 718 was investigated, focusing on the conditions that may lead to the development of very large grains (about 100 lm) in a recrystallized fine grained matrix (4 to 5 lm) despite the presence of second-phase particles. Microstructure evolution was analyzed by EBSD (grain size, intragranular misorientation) and SEM (d phase par...
متن کاملTransmission Electron Microscopy Sample Preparation of INCONEL 738 Nickel-Base Superalloy
Size, shape, volume fraction and distribution of embedded g/ phase in g phase has direct effect on strength of INCONEL alloy. Microstructure parameters of INCONEL phases are quantified from microstructure images using transmission electron microscopy (TEM). Different TEM sample preparation techniques were used to study INCONEL 738 alloy microstructure for transmission electron micros...