High-aspect-ratio bulk micromachining of titanium.

Recent process developments have permitted the highly anisotropic bulk micromachining of titanium microelectromechanical systems (MEMS). By using the metal anisotropic reactive ion etching with oxidation (MARIO) process, arbitrarily high-aspect-ratio structures with straight sidewalls and micrometre-scale features have been bulk micromachined into titanium substrates of various thicknesses, ran...

متن کامل

SYNTHESIS OF HIGH ASPECT RATIO SILVER NANOWIRES: PARAMETRIC STUDY OF THE POLYOL PROCESS

Silver nanowires (AgNWs) are considered as one-dimensional nanostructures, which have received much attention due to their nanoscale size, high aspect ratio, high electrical and thermal conductivity, optical transparency and high mechanical stability. Preparation of AgNWs by polyol process is remarkably sensitive to the interactions between synthesis parameters. In this study, the effect of the...

متن کامل

Approaches to High Aspect Ratio Triangulations

In aerospace computational uid dynamics calculations, high aspect ratio, or stretched, triangulations are often used to adequately resolve the features of a viscous ow around bodies. In this paper, we explore alternatives to the Delaunay triangulation which can be used to generate high aspect ratio triangulations of point sets. The method is based on a variation of the lifting map concept which...

متن کامل

High Aspect Ratio Si Etching in STS2

Deep reactive ion etching (DRIE) is one of the most important etching techniques because it is independent of crystal orientation and does not require any wet process. DRIE can be applied for many applications. For examples, this technique can be used to fabricate MEMS devices (e.g. accelerometers, scanners, etc.), microfluidic devices, electrical through wafer interconnects, and so on. In many...

متن کامل

High aspect-ratio polysilicon micromachining technology

This paper presents a single wafer, all-silicon, high aspect-ratio multi-layer polysilicon micromachining technology that combines deep dry etching of silicon with conventional surface micromachining to realize tens to hundreds of microns thick, high aspect-ratio, electrically isolated polysilicon structures with sub-micron air-gaps. Vertical polysilicon sense electrodes as tall as the main bod...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Japan Society for Precision Engineering

سال: 2009

ISSN: 1882-675X,0912-0289

DOI: 10.2493/jjspe.75.1083