Very High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4
The effect of casting pores on the very high cycle fatigue (VHCF) behavior of a directionally solidified (DS) Ni-base superalloy DZ4 is investigated. Casting and hot isostatic pressing (HIP) specimens were subjected to very high cycle fatigue loading in an ambient atmosphere. The results demonstrated that the continuously descending S-N curves were exhibited for both the casting and HIP specime...
متن کاملThermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...
متن کاملHold-time Effects on Low-cycle-fatigue Behavior of Hastelloy® X Superalloy at High Temperatures
Total strain-controlled low-cycle-fatigue tests with and without hold times were performed at temperatures ranging from 816°C to 982°C in a laboratory air on a nickel-based superalloy, HASTELLOY X. The influence of hold times on the cyclicstress response and fatigue life was studied. At the temperatures considered, the alloy exhibited initial cyclic hardening, followed by a saturated cyclic-str...
متن کاملThe Ballistic Behavior of High Strength, Low Alloy-100 Steel at Sub-zero Temperatures
The ballistic response of the high strength, low alloy (HSLA-100) steel at ambient and temperatures of -400°C, -800°C and -1960°C is investigated in this work. Lambert-jonas equation is used to fit the experimental results into a curve. The effect of quenching on ballistic behavior of HSLA-100 is also studied. The experiments are conducted on 3mm thick rectangular specimens impacted by blunt ti...
متن کاملHigh Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 1997
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.46.32