Hydrogen-plasticity interactions in pearlitic steel: A fractographic and numerical study
نویسندگان
چکیده
منابع مشابه
Study on Corrosion Behavior of Pearlitic Rail Steel
The present study is an attempt to find out the effect of environmental corrosion on the commonly used pearlitic rail steel. The cases of corrosion of rail under Indian environment have been studied. It has been found that in marine environment both the yield strength and tensile strength decreases with increasing corrosion rate. In acidic environment yield strength increased with increasing co...
متن کاملHydrogen Assisted Cracking in Pearlitic Steel Rods: The Role of Residual Stresses Generated by Fatigue Precracking
Stress corrosion cracking (SCC) of metals is an issue of major concern in engineering since this phenomenon causes many catastrophic failures of structural components in aggressive environments. SCC is even more harmful under cathodic conditions promoting the phenomenon known as hydrogen assisted cracking (HAC), hydrogen assisted fracture (HAF) or hydrogen embrittlement (HE). A common way to as...
متن کاملAnalysis of Fatigue Crack Paths in Cold Drawn Pearlitic Steel
In this paper, a fracto-metallographic analysis was performed on the cracked specimens of cold drawn pearlitic steel subjected to fatigue tests. Fatigue cracks are transcollonial and exhibit a preference for fracturing pearlitic lamellae, with non-uniform crack opening displacement values, micro-discontinuities, branchings, bifurcations and frequent local deflections that create microstructural...
متن کاملFractographic Investigation of Failure in Stainless Steel Orthopedic Plates
Plates of austenitic stainless steel are often used in orthopedic surgery for fixing ends of the broken bones and for repairing fractures. The paper analyzes a premature breakage of six plates for fixing broken bones with different patients during their recovery. Each plate's breakage can induce serious aftermaths such as a new surgery, unexpected undesired complications and a prolonged healing...
متن کاملa study on rate making and required reserves determination in reinsurance market: a simulation
reinsurance is widely recognized as an important instrument in the capital management of an insurance company as well as its risk management tool. this thesis is intended to determine premium rates for different types of reinsurance policies. also, given the fact that the reinsurance coverage of every company depends upon its reserves, so different types of reserves and the method of their calc...
ذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science and Engineering: A
سال: 1996
ISSN: 0921-5093
DOI: 10.1016/s0921-5093(96)10425-1