Influence of homogenization degree on microstructure and mechanical properties for a novel wrought superalloy
نویسندگان
چکیده
Abstract The present work aims at investigating the impact of homogenization time on microstructure and mechanical properties a Ni-based superalloy GH4151 during hot deformation. results showed that dense dendrite structure remained after 1200°C for 5 h, which was similar to as-cast microstructure. Higher flow stress cracking in h-homogenized material is attributed integral deformation with greater resistance less recrystallization. Furthermore, decrease increasing helped promote dynamic recrystallization (DRX) 12h 36 h due nucleation position. When increased 60h, increase grain size makes dislocation gather within increase.
منابع مشابه
The Influence of Homogenization and Solution Annealing Process on the Microstructure and Mechanical Properties of 1.4470 Ferritic-austenitic Stainless Steel
In the present research, the effect of the homogenization process and annealing temperature were investigated for the 1.4470 ferritic-austenitic stainless steel in the as-cast condition. In this regard, microstructural evolutions, hardness, and impact energy of the steel was evaluated with different heat treatment conditions. The results show that the minimum volume fraction of austenite phase ...
متن کاملdetermination of some physical and mechanical properties red bean
چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...
15 صفحه اولInfluence of Cu and Ni on the Microstructure and Mechanical Properties of an HSLA Steel
In this research the role of alloying elements on the microstructure and mechanical properties of an as cast and hot rolled high strength low alloy (HSLA) steel was studied. Different compositions with different amount of copper in the presence of nickel, hot rolled and quenched in oil. Tensile test, hardness test, scanning electron microscope (SEM) and optical microscope (OM) were used to eval...
متن کاملInfluence of Rolling on Microstructure and Mechanical Properties of Bronze-Steel Explosive Welded Sheets
In this paper, the microstructure and mechanical properties of the plain carbon steel-bronze interface of explosive welding and rolling were investigated. Explosive connection was done at two stop distances and with two different thicknesses of explosive material. Rolling of the welded composite was done at both ambient and preheated temperatures of 300 °C and with a constant thickness reductio...
متن کاملInfluence of Rolling on Microstructure and Mechanical Properties of Bronze-Steel Explosive Welded Sheets
In this paper, the microstructure and mechanical properties of the plain carbon steel-bronze interface of explosive welding and rolling were investigated. Explosive connection was done at two stop distances and with two different thicknesses of explosive material. Rolling of the welded composite was done at both ambient and preheated temperatures of 300 °C and with a constant thickness reductio...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of physics
سال: 2023
ISSN: ['0022-3700', '1747-3721', '0368-3508', '1747-3713']
DOI: https://doi.org/10.1088/1742-6596/2519/1/012040