Influence of Micro-Arc Oxidation Coatings on Stress Corrosion of AlMg6 Alloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of KMnO4 Concentrationon Infrared Emissivity of Coatings Formed on TC4 Alloys by Micro-Arc Oxidation

Ceramic coatings with high emissivity were fabricated on TC4 alloys by micro-arc oxidation technique (MAO) in mixed silicate and phosphate electrolytes with varying KMnO₄ addition. The microstructure, phase and chemical composition were characterized by scanning electron microscope (SEM), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS), and the infrared emissivity of the MAO...

متن کامل

Effect of Plasma Electrolytic Oxidation Process as a Pretreatment on Corrosion Resistance of Polymeric Coatings Applied on Mg Alloy

In this study, Plasma Electrolytic Oxidation (PEO) at three frequencies of 500, 1000 and 3000 Hz was applied on Mg surface and the effect of PEO surface preparation on protective behavior of three types of epoxy, fusion bond epoxy (FBE) and polyurethane coatings was investigated. The microstructural and protective properties of PEO coatings were studied by SEM, potentiodynamic polarization and ...

متن کامل

Effect of Plasma Electrolytic Oxidation Process as a Pretreatment on Corrosion Resistance of Polymeric Coatings Applied on Mg Alloy

In this study, Plasma Electrolytic Oxidation (PEO) at three frequencies of 500, 1000 and 3000 Hz was applied on Mg surface and the effect of PEO surface preparation on protective behavior of three types of epoxy, fusion bond epoxy (FBE) and polyurethane coatings was investigated. The microstructural and protective properties of PEO coatings were studied by SEM, potentiodynamic polarization and ...

متن کامل

Formation and Corrosion Resistance of Micro-Arc Oxidation Coating on Equal-Channel Angular Pressed AZ91D Mg Alloy

Aibin Ma 1,2,*, Fumin Lu 1, Qi Zhou 1, Jinghua Jiang 1,*, Dan Song 1,2, Jianqing Chen 1 and Yuxi Zheng 1 1 College of Mechanics and Materials, Hohai University, Nanjing 210098, China; [email protected] (F.L.); [email protected] (Q.Z.); [email protected] (D.S.); [email protected] (J.C.); [email protected] (Y.Z.) 2 Suqian Institute, Hohai University, Suqian 223800, China * Correspondence: ai...

متن کامل

Characterization of hydroxyapatite containing micro-arc oxidation coating on ZK60 magnesium alloy

INTRODUCTION: Magnesium alloys are attractive as a class of biodegradable metallic materials. However, too fast degradation is an obstacle to their clinical applications. Recently, micro-arc oxidation (MAO) coatings were applied on biodegradable magnesium alloys to delay their degradation. In vivo studies showed that the protective ability of the MAO coating should be further improved [1]. Seal...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials

سال: 2020

ISSN: 1996-1944

DOI: 10.3390/ma13020356