Influence of Thermal Cycles Number on Bond Strength of Metallic Brackets to Ceramic

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic.

This study investigated the influence of water storage (24 h and 6 months), and Transbond XT and Fuji Ortho LC bonding materials on the bond strength of metallic brackets bonded to feldspathic ceramic. Four cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 60 s. Each cylinder received two layers of silane. Metallic brackets were bonded to the cylinders using Transbond ...

متن کامل

Shear Bond Strength of Metallic Brackets: Influence of Saliva Contamination

OBJECTIVE To evaluate the influence of saliva contamination on shear bond strength and the bond failure pattern of 3 adhesive systems (Transbond XT, AdheSE and Xeno III) on orthodontic metallic brackets bonded to human enamel. MATERIAL AND METHODS Seventy-two permanent human molars were cut longitudinally in a mesiodistal direction, producing seventy-two specimens randomly divided into six gr...

متن کامل

Effect of etching time and light source on the bond strength of metallic brackets to ceramic.

This study evaluated the bond strength of brackets to ceramic testing different etching times and light sources for photo-activation of the bonding agent. Cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 20 or 60 s. After application of silane on the ceramic surface, metallic brackets were bonded to the cylinders using Transbond XT (3M Unitek). The specimens for each ...

متن کامل

Effect of Acid Etching, Silane and Thermal Cycling on the Bond Strength of Metallic Brackets to Ceramic.

The aim of this study was to evaluate the effect of silanes, thermal cycling and acid etching on the shear bond strength (SBS) of metallic brackets to feldspathic ceramic. Feldspathic ceramic cylinders (Groups 1, 2, 5 and 6) were etched for 60 s with 10% hydrofluoric acid and Groups 3, 4, 7 and 8, without acid etching. Two layers of silane Clearfil Ceramic Primer (CCP, Groups 1 to 4) and two la...

متن کامل

Influence of various surface-conditioning methods on the bond strength of metal brackets to ceramic surfaces.

With the increase in adult orthodontic treatment comes the need to find a reliable method for bonding orthodontic brackets onto metal or ceramic crowns and fixed partial dentures. In this study, shear bond strength and surface roughness tests were used to examine the effect of 4 different surface conditioning methods: fine diamond bur, sandblasting, 5% hydrofluoric acid, and silica coating for ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید