Intensified chipping during nanoindentation and the effect of friction on the interfacial fracture for thin films used in N/MEMS
نویسندگان
چکیده
Abstract Nanoindentation was performed on Ti-B-Si-C and SiCN films deposited Si substrates at varying loads depths of penetrations. The intensity chipping got enhanced with an increasing load which represented geometrically. pop-in pop-out events occurring in the unloading were explained as cracking high-pressure phase transformation. interfacial fracture stability adhesion film-substrate system, crucial for N/MEMS devices analyzed respect to frictional coefficient help Finite Element Modelling (FEM).
منابع مشابه
the effect of e-64 on the developmental competence of sheep cocs during in vitro maturation
in the present study, the effect of e-64 at different concentrations (0.5, 1, 5 and 10 µm) added to (1) the ivm medium on oocyte nuclear maturation and developmental competence of ovine oocytes, and (2) to the ivc medium on embryonic development of ovine embryos were investigated.
the analysis of the role of the speech acts theory in translating and dubbing hollywood films
از محوری ترین اثراتی که یک فیلم سینمایی ایجاد می کند دیالوگ هایی است که هنرپیش گان فیلم میگویند. به زعم یک فیلم ساز, یک شیوه متأثر نمودن مخاطب از اثر منظوره نیروی گفتارهای گوینده, مثل نیروی عاطفی, ترس آور, غم انگیز, هیجان انگیز و غیره, است. این مطالعه به بررسی این مسأله مبادرت کرده است که آیا نیروی فراگفتاری هنرپیش گان به مثابه ی اعمال گفتاری در پنج فیلم هالیوودی در نسخه های دوبله شده باز تولید...
15 صفحه اولthe washback effect of discretepoint vs. integrative tests on the retention of content in knowledge tests
در این پایان نامه تاثیر دو نوع تست جزیی نگر و کلی نگر بر به یادسپاری محتوا ارزیابی شده که نتایج نشان دهندهکارایی تستهای کلی نگر بیشتر از سایر آزمونها است
15 صفحه اولthe effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)
cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...
“the effect of risk aversion on the demand for life insurance: the case of iranian life insurance market”
abstract: about 60% of total premium of insurance industry is pertained?to life policies in the world; while the life insurance total premium in iran is less than 6% of total premium in insurance industry in 2008 (sigma, no 3/2009). among the reasons that discourage the life insurance industry is the problem of adverse selection. adverse selection theory describes a situation where the inf...
15 صفحه اولذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Engineering research express
سال: 2022
ISSN: ['2631-8695']
DOI: https://doi.org/10.1088/2631-8695/ac9c85