Interfacial Microstructure of SiC/Cu Joint Friction-Bonded with Ti Intermediate Layer

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Study the Profile Shape and Mechanical Properties of Bonded Joint HNV3 to Nimonic 80A Superalloy with Inertia Friction Welding Method

This Paper presents the welding parameterchr('39')s effect (forging pressure, welding time) on macrostructure and mechanical properties of friction welding valve steel HNV3 to Nimonic 80A super alloy. For this purpose, two rods with 20 mm diameters are prepared and with using different parameters (Increase forging pressure and welding time) by friction welding method are welded together. Tensil...

متن کامل

Study the Profile Shape and Mechanical Properties of Bonded Joint HNV3 to Nimonic 80A Superalloy with Inertia Friction Welding Method

This Paper presents the welding parameterchr('39')s effect (forging pressure, welding time) on macrostructure and mechanical properties of friction welding valve steel HNV3 to Nimonic 80A super alloy. For this purpose, two rods with 20 mm diameters are prepared and with using different parameters (Increase forging pressure and welding time) by friction welding method are welded together. Tensil...

متن کامل

Microstructure and Mechanical Properties of the Friction Welded Joint between X53CrMnNiN219 and X45CrSi93 Stainless Steel

Dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. In this study, X53CrMnNiN219 (austenitic stainless steel) and X45CrSi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. The welded joint was then heat treated at 760 0C for 60 min. Mechanical prop...

متن کامل

Analysis of adhesive-bonded single-lap joint with an interfacial crack and a void

void within the adhesive. Depending upon the number of notches and voids, the specimen is divided into several regions. Assuming that a plane strain state of deformation prevails in the specimen, we write the balance of forces and moments for each section and impose the continuity of displacements, forces and moments at the interfaces between the adjoining sections. By taking the Laplace transf...

متن کامل

microstructure and mechanical properties of the friction welded joint between x53crmnnin219 and x45crsi93 stainless steel

dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. in this study, x53crmnnin219 (austenitic stainless steel) and x45crsi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. the welded joint was then heat treated at 760 0c for 60 min. mechanical prop...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Japan Institute of Metals and Materials

سال: 2003

ISSN: 0021-4876,1880-6880

DOI: 10.2320/jinstmet1952.67.10_538