Keyhole TIG welding of newly developed nickel-based superalloy VDM Alloy 780

نویسندگان

چکیده

Abstract The influence of keyhole TIG (K-TIG) welding parameters on the weld geometry and defects a new nickel-based superalloy VDM Alloy 780 alloy were investigated using statistical design experiment, microstructures heat-affected zone (HAZ) fusion (FZ) K-TIG-welded characterized. No cracks are found in FZ HAZ. Travel speed significantly influences minimum width (Wm), face root excess metal, underfill, average pore diameter. Welding current interaction current*travel metals, respectively. Interdendritic microconstituents identified as (Nb,Ti)C particles γ/Laves eutectic constituents based SEM–EDS analysis. In addition, plate-like precipitates likely to be δ/η phase observed surrounding interdendritic Laves eutectics, γ′ inhomogeneously precipitated FZ. partially melted (PMZ), (Nb,Ti)C, phase, liquated resolidified regions. Constitutional liquation HAZ is where appears associated with product.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Tig Welding Process Pdf

Tungsten inert gas (TIG) welding, also called as gas tungsten welding 1. (a) Schematic of TIG welding Process (b) Variety of tungsten electrodes. The activated TIG (ATIG) welding process mainly focuses on increasing the depth of penetration and the reduction in the width of weld bead has not been paid. Tungsten inert gas welding, TIG is widely applied in manufacturing process for different The ...

متن کامل

Effect of welding parameters on penetration depth in FB-TIG welding of 5083 aluminum alloy

In the present study, effect of current, welding speed and preheat temperature during FB-TIG welding of AA5083 aluminum alloy was studied. Using the Taguchi method, 9 different tests were designed to investigate the effect of welding parameters on the penetration depth. Consistent with predictions, increasing the current and preheat temperature, and reducing the welding speed led to an increase...

متن کامل

Effect of welding parameters on penetration depth in FB-TIG welding of 5083 aluminum alloy

In the present study, effect of current, welding speed and preheat temperature during FB-TIG welding of AA5083 aluminum alloy was studied. Using the Taguchi method, 9 different tests were designed to investigate the effect of welding parameters on the penetration depth. Consistent with predictions, increasing the current and preheat temperature, and reducing the welding speed led to an increase...

متن کامل

Diffusion Welding of Nickel-based Superalloys

Ni based superalloys can be welded by diffusion bonding. Temperature, diffusion coefficient, activation energy and Boltzmann constant influence the quality of diffusion bonding, so obtaining the best condition for welding is considered. Showing the suitable condition for diffusion welding of nickel-based superalloys is the aim of this paper.

متن کامل

Control of dynamic keyhole welding process

Weld joint penetration control is a basic research topic in the welding research community. The authors propose using an innovative plasma arc welding process referred to as the quasi-keyhole process to achieve less application-dependent weld joint penetration sensing and control. To control the quasi-keyhole process, the peak current and keyhole sustaining current are selected as the control v...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Welding in The World

سال: 2022

ISSN: ['0043-2288', '1878-6669']

DOI: https://doi.org/10.1007/s40194-022-01425-y