Kinetics and Mechanisms of γ′ Reprecipitation in a Ni-based Superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Kinetics and Mechanisms of γ′ Reprecipitation in a Ni-based Superalloy

The reprecipitation mechanisms and kinetics of γ' particles during cooling from supersolvus and subsolvus temperatures were studied in AD730(TM) Ni-based superalloy using Differential Thermal Analysis (DTA). The evolution in the morphology and distribution of reprecipitated γ' particles was investigated using Field Emission Gun Scanning Electron Microscopy (FEG-SEM). Depending on the cooling ra...

متن کامل

Dislocation network with pair-coupling structure in {111} γ/γ′ interface of Ni-based single crystal superalloy

The γ/γ' interface dislocation network is reported to improve the high temperature creep resistance of single crystal superalloys and is usually found to deposit in {001} interface. In this work, a new type of dislocation network was found in {111} γ/γ' interface at a single crystal model superalloy crept at 1100 °C/100 MPa. The dislocations in the network are screw with Burgers vectors of 1/2 ...

متن کامل

Hot Ductility Loss in a Fe-Ni-Based Superalloy

High temperature tensile tests have been conducted on samples of a Fe-Ni based superalloy, Incoloy A-286, and significant ductility loss has been observed at 1220 °C. Titanium-rich, thin-film-like phase has been found on the inter-granular facets of fracture surfaces. It appears that sulfur content of Ti-rich phase was higher than that of the matrix. At 1220 °C, liquation of Ti-rich phases has ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Scientific Reports

سال: 2016

ISSN: 2045-2322

DOI: 10.1038/srep28650