Mechanical characterization of crosslinking effect in polydimethylsiloxane using nanoindentation

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanical characterization of magnetic nanowire–polydimethylsiloxane composites

One-dimensional magnetic nanowires have been introduced into polydimethylsiloxane PDMS to form polymer based nanocomposites. In contrast to the conventional nanofillers such as carbon nanotubes, carbon nanofibers, nanoparticles, and layer-structured materials, these well-defined anisotropic metallic nanowires are highly conductive and have much weaker van der Waals interactions. Moreover, compo...

متن کامل

Advances in the mechanical characterization of soft materials by nanoindentation

The emergence of nanoscience has spurred the demand for technologies capable of probing physical phenomena at resolutions down to the atomic length scale. Under this initiative, recent advances in instrumented nanoindentation have made the atomic force microscope and the depth-sensing nanoindenter practical tools in studying the local material properties of a broad array of solid surfaces at mi...

متن کامل

Obtaining full contact for measuring polydimethylsiloxane mechanical properties with flat punch nanoindentation

Procedure to establish full contact between the sample and the 1 mm diameter cylindrical flat punch tip to measure polydimethylsiloxane (PDMS) mechanical properties using the Hysitron TriboIndenter is described. This procedure differs from the standard automated indentation because each indent has to be performed manually after establishing full contact with the sample surface. Incomplete conta...

متن کامل

Mechanical Characterization of the Heat Affected Zone of Gold Wirebonds Using Nanoindentation

Abstrac t -With increasing miniaturization in microelectronics the wirebonds used in IC packages are witnessing a thrust towards fine pitch wirebonding. To have a precise control over loop height of the wirebond for fine pitch wirebonding, it is imperative to do mechanical characterization of the wirebond. The present work studies the mechanical properties of gold wire and wirebond using nanoin...

متن کامل

Time-dependent mechanical characterization of poly(2-hydroxyethyl methacrylate) hydrogels using nanoindentation and unconfined compression.

Hydrogels pose unique challenges to nanoindentation including sample preparation, control of experimental parameters, and limitations imposed by mechanical testing instruments and data analysis originally intended for harder materials. The artifacts that occur during nanoindentation of hydrated samples have been described, but the material properties obtained from hydrated nanoindentation have ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Polymer Testing

سال: 2016

ISSN: 0142-9418

DOI: 10.1016/j.polymertesting.2016.10.034